Armor steel with excellent bendability.
Armox® 370T Class 2 is a rolled homogeneous armor plate (RHA) that combines good resistance to penetration with excellent toughness.
Benefits of Armox® 370T Class 2 include:
Armox® 370T Class 2 is not intended for further heat treatment.
Thickness (mm) |
Hardness (HBW) |
Yield strength Rp0.2 (min MPa) |
Tensile strength Rm (MPa) |
Elongation A5 (min %) |
Elongation A50 (min %) |
---|---|---|---|---|---|
3.0 - 5.9 | 280 - 330 | 800 | 900 - 1100 | 13 | 15 |
6.0 - 59.9 | 280 - 330 | 800 | 900 - 1100 | 13 | 15 |
60.0 - 100.0 | 280 - 330 | — | — | — | — |
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.
Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.
Tensile test according to EN ISO 6892 on each heat and thickness under 60 mm.
According to EN ISO 10160 Class E3S3 for thicknesses up to 80 mm and E1S2 for > 80 mm.
Thickness (mm) |
Min impact energy for transversal testing, Charpy V 10x10 mm test specimen 1) |
---|---|
6.0 - 100.0 | 60 J / -40 °C |
1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.
C *) (max %) |
Si *) (max %) |
Mn*) (max %) |
P (max %) |
S (max %) |
Cr*) (max %) |
Ni*) (max %) |
Mo*) (max %) |
B*) (max %) |
---|---|---|---|---|---|---|---|---|
0.32 | 0.40 | 1.20 | 0.010 | 0.003 | 1.0 | 1.80 | 0.70 | 0.005 |
The steel is grain-refined. *) Intentional alloying elements.
More details are given in SSAB´s brochure Armox® Guarantees or on www.ssab.com.
Thickness (mm) | Tolerance (mm) |
---|---|
3.0 - 12.9 | - 0.0 / + 0.8 |
13.0 - 19.9 | - 0.0 / + 1.0 |
20.0 - 39.9 | - 0.0 / + 1.2 |
40.0 - 59.9 | - 0.0 / + 1.6 |
60.0 - 79.9 | - 0.0 / + 2.0 |
80.0 - 100.0 | - 0.0 / + 2.4 |
According to SSAB´s dimension program.
Tolerances according to EN 10029.
Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).
According to EN 10163-2 Class B Subclass 3.
The delivery condition is QT (Quenched and Tempered).