High reliability high versatility

SSAB Domex® comes as hot rolled plate, hot or cold rolled strip, tubes and sections. It’s also available in different metal-coated grades for corrosion resistance with zinc, galfan and galvannealed coatings.

Contact sales

    Hot rolled strip

    Hide/Show specific columns Edit
    Select columns to display
      Product Name Dimensions Standards Datasheet
      SSAB Domex 240YP T: 1.80 - 20.00 mm
      W: Up to 1860 mm
      EN 10025-2

      SSAB Domex® 240YP

      SSAB Domex 315MC T: 1.80 - 18.00 mm
      W: Up to 1860 mm
      EN 10149-2

      SSAB Domex® 315MC

      SSAB Domex 355MC T: 1.80 - 16.00 mm
      W: Up to 1860 mm
      EN 10149-2

      SSAB Domex® 355MC

      SSAB Domex 420MC T: 1.80 - 15.00 mm
      W: Up to 1800 mm
      EN 10149-2

      SSAB Domex® 420MC

      SSAB Domex 460MC T: 2.00 - 13.00 mm
      W: Up to 1800 mm
      EN 10149-2

      SSAB Domex® 460MC

      SSAB Domex 500MC T: 2.00 - 13.00 mm
      W: Up to 1800 mm
      EN 10149-2

      SSAB Domex® 500MC

      SSAB Domex 550MC T: 2.00 - 12.80 mm
      W: Up to 1640 mm
      EN 10149-2

      SSAB Domex® 550MC

      SSAB Domex 355MC Plus T: 3.00 - 12.00 mm
      W: Up to 1860 mm
      EN 10149-2

      SSAB Domex® 355 MC Plus

      SSAB Domex 420MC Plus T: 3.00 - 10.00 mm
      W: Up to 1860 mm
      EN 10149-2

      SSAB Domex® 420MC Plus

      SSAB Domex 460MC Plus T: 4.00 - 10.00 mm
      W: Up to 1800 mm
      EN 10149-2

      SSAB Domex® 460MC Plus

      SSAB Domex 500MC Plus T: 3.00 - 8.00 mm
      W: Up to 1800 mm
      EN 10149-2

      SSAB Domex® 500MC Plus

      Compare parameters

      Select one parameter to compare

      Comparison

        Cold rolled strip

        Hide/Show specific columns Edit
        Select columns to display
          Product Name Dimensions Standards Datasheet
          SSAB Domex® 260LA T: 0.40 - 3.00 mm
          W: Up to 1500 mm
          EN 10268

          SSAB Domex® 260LA

          SSAB Domex® 300LA T: 0.40 - 3.00 mm
          W: Up to 1500 mm
          EN 10268

          SSAB Domex® 300LA

          SSAB Domex® 340LA T: 0.40 - 3.00 mm
          W: Up to 1500 mm
          EN 10268

          SSAB Domex® 340LA

          SSAB Domex® 380LA T: 0.45 - 3.00 mm
          W: Up to 1500 mm
          EN 10268

          SSAB Domex® 380LA

          Compare parameters

          Select one parameter to compare

          Comparison

            Metal-coated strip

            Hide/Show specific columns Edit
            Select columns to display
              Product Name Dimensions Standards Datasheet
              SSAB Domex® 220LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              SSAB

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 260LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 300LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 340LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 380LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 420LAD T: 0.50 - 3.00 mm
              W: Up to 1520 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 460LAD T: 0.80 - 3.00 mm
              W: Up to 1500 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              SSAB Domex® 500LAD T: 0.80 - 2.00 mm
              W: Up to 1410 mm
              EN 10346

              SSAB Domex® - Metal coated HSLA steels

              Compare parameters

              Select one parameter to compare

              Comparison

                Tubes and sections

                Hide/Show specific columns Edit
                Select columns to display
                  Product Name Dimensions Standards Datasheet
                  SSAB Domex Tube 460MH Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.5 mm
                  EN 10219-1, EN 10219-2
                  SSAB Domex Tube 500MH Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.5 mm
                  EN 10219-2, EN 1090-2
                  SSAB Domex Tube 550MH Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.50 mm
                  EN 10219-2, EN 1090-2
                  SSAB Domex Tube Double Grade Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.50 mm
                  EN 10219-1, EN 10219-2
                  Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.50 mm
                  EN 10219-1, EN 10219-2
                  SSAB Domex Tube 235 JRH Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.50 mm
                  EN 10219-1, EN 10219-2
                  SSAB Domex Tube 355J2H Circular: 42.4 - 323.9 mm
                  Square: 40x40 - 300x300 mm
                  Rectangular: 50x30 - 400x200 mm
                  Wall Thickness: 2.0 - 12.5 mm
                  EN 10219-1, EN 10219-2
                  Compare parameters

                  Select one parameter to compare

                  Comparison