Strenx® 900 product group

Strenx® 900 is a group of high-strength structural steel grades with yield strengths between 830 and 900 MPa (120-130 ksi) depending on thickness, making them an excellent choice for transport, lifting, agriculture and other load-bearing applications.

SUITABLE APPLICATIONS
Advanced load-bearing structures in transportation, lifting and agriculture

TYPE OF PRODUCTS
Hot rolled plate and sheet

THICKNESS RANGE
2-120 mm (0.079”-4.724”)

High-strength steel grades for high-performing structural applications

STRENX® 900 E
Superior toughness

Suitable for strong and light chassis, cranes, agriculture equipment and other load-bearing structures in a wide dimension range.

Toughness: 27 J at -40°C ( 20 ft-lb at -40°F)
Thickness: 4-120 mm (0.157”-4.724”)
Standard: EN 10025-6 S890QL
Format: Plate

Go to product page

STRENX® 900 F
Extreme toughness in cold conditions

Suitable for strong and light chassis, cranes, agriculture equipment and other load-bearing structures, particularly in cold conditions.

Toughness: 27 J at -60 °C (20 ft-lb at -76 °F)
Plate: 4-100 mm (0.157”- 3.937”)
Standard:EN 10025-6 S890QL1
Format: Plate

Go to product page

STRENX® 900 MC
Hot rolled steel for cold forming

Excellent thickness accuracy and surface quality for predictable performance in cold forming operations.

Toughness: 27 J at -40°C (20 ft-lb at -40°F)
Thickness: 3-10 mm (0.118”-0.393”)
Standard: EN 10149-2 S900MC
Format: Sheet and coil

Go to product page

STRENX® 900 PLUS
Superior bendability

Suitable for strong and light chassis, cranes, agriculture equipment and other load-bearing structures.

Toughness: 27 J at -40°C (20 ft-lb at -40°F)
Thickness: 2-8 mm (0.079”-0.315”)
Standard: EN 10025-6 S890QL
Format: Sheet and coil

Go to product page
Strenx 900

Concrete pump manufacturer Betonstar upgraded to Strenx® 900, saved weight and reached longer

“The fact that the pumps weigh less provides many advantages, like less fuel consumption, the possibility of purchasing trucks with a shorter wheelbase, and pouring concrete usingless fuel – and, of course, less fuel is consumed when you drive a lighter truck,” says Erol Yıldız, factory manager at Betonstar.

Read the full case

Made for predictable performance in the workshop

Person welding Strenx® high-strength steel in the workshop.

Welding

Strenx® 900 can be welded using any conventional welding method. MAG welding is the most common technique today, since it is very easy to automate for high productivity.

Strenx machining

Machining

Strenx® 900 can usually be machined without special equipment. Stable machinery fitted with high-speed steel and carbide tools is recommended when drilling, countersinking, tapping, turning, and milling.

Strenx bending

Bending

Free bending and roll bending of Strenx® steel plate and strip can be done using standard bending machinery. Uniform properties, close thickness tolerances and high surface quality ensure a predictable bending process.

Strenx thermal cutting

Thermal cutting

The properties and fine surface finish of Strenx® 900 plate and sheet make it perfect for laser cutting. Thermal cutting of hot rolled Strenx® 900 is performed with oxy-fuel flame, plasma and laser.

Strenx mechanical cutting

Mechanical cutting

Mechanical cutting of Strenx® 900 is best performed with guillotine shears. Consider carefully the settings of the cutting machine. The most important factors are clearance, cutting angle and blade hardness. The plate should be allowed to warm up thoroughly to around +20°C (68° F) before it is cut.

Strenx guarantees

Strenx® guarantees

Strenx® guarantees include tight thickness tolerances, tight flatness tolerances and bending properties. The tight thickness tolerances enable you to know the weight more precisely. As a result, you can reduce your safety margins. Precise thickness within a plate and between plates makes for safe and predictable performance in the workshop.

Learn more about your guarantees

Strenx® 900 products and thickness

Strenx® 900 Standard Products

Strenx® 900 E

Thickness range [mm]
Plate
4-120
Thickness range [mm]
Hot rolled
strip
---
Thickness range [mm]
Cold rolled
strip
---
Conform to standard
S890QL in EN 10025-6 Impact test at -40°C
Formats
Plates
Typical products manufactured
with Strenx®
Lifting and load-bearing structures, where strength and weight is critical
Strenx® 900 Standard Products

Strenx® 900 F

Thickness range [mm]
Plate
4-100
Thickness range [mm]
Hot rolled
strip
---
Thickness range [mm]
Cold rolled
strip
---
Conform to standard
S890QL1 in EN 10025-6 Impact test at -60°C
Formats
Plates
Typical products manufactured
with Strenx®
Lifting and load-bearing structures, where strength and weight is critical in cold conditions
Strenx® 900 Standard Products

Strenx® 900 MC

Thickness range [mm]
Plate
---
Thickness range [mm]
Hot rolled
strip
3-10
Thickness range [mm]
Cold rolled
strip
---
Conform to standard
S900MC in EN 10149-2 Impact test at -40°C
Formats
Sheets & Coils
Typical products manufactured
with Strenx®
Load-bearing structures, where strength and weight is critical
Strenx® 900 Standard Products

Strenx® 900 Plus

Thickness range [mm]
Plate
---
Thickness range [mm]
Hot rolled
strip
2-8
Thickness range [mm]
Cold rolled
strip
---
Conform to standard
S890QL in EN 10025-6 Impact test at -40°C
Formats
Sheets &  Coils
Typical products manufactured
with Strenx®
Lifting and load-bearing structures, where strength and weight is critical
Copyright 2026