    General Product Description

    GreenCoat Cool color coated steel is available in regular gloss. It is used in roofing and features special solar heat reflecting properties that make the surface stay cooler than regular coated surfaces. For buildings that need cooling, this product helps to save energy and increase the thermal comfort. The largest difference in surface temperature between GreenCoat Cool and standard products is achieved for dark colors.

    GreenCoat Cool color coated steel offers a coating that is optimized to resist corrosion (RC5). The structured surface helps to protect against mechanical wear and is easy to handle during manufacturing. The reverse side of the sheet is painted with a two-layer grey backside coating.

    GreenCoat Cool complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Regular
      Gloss 40
      Minimum inner bending radius 1.0 x sheet thickness
      Scratch resistance 35 N
      UV radiation resistance RUV3
      Corrosion resistance 1) RC5
      Stain resistance Excellent
      Highest operating temperature 100 °C
      Coating thickness, nominal (primer + top coat) 40 µm
      Coating structure Structured
      Steel designation 2) S280GD, S320GD, S350GD
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.50 mm
      Steel width 2) 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Regular
        40
        Technical Properties
        Minimum inner bending radius
        Regular
        1.0 x sheet thickness
        Technical Properties
        Scratch resistance
        Regular
        35 N
        Technical Properties
        UV radiation resistance
        Regular
        RUV3
        Technical Properties
        Corrosion resistance 1)
        Regular
        RC5
        Technical Properties
        Stain resistance
        Regular
        Excellent
        Technical Properties
        Highest operating temperature
        Regular
        100 °C
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Regular
        40 µm
        Technical Properties
        Coating structure
        Regular
        Structured
        Technical Properties
        Steel designation 2)
        Regular
        S280GD, S320GD, S350GD
        Technical Properties
        Zinc coating
        Regular
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Regular
        0.50 mm
        Technical Properties
        Steel width 2)
        Regular
        1000 - 1500 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

        5 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat Cool

        Anthracite Grey

        RR2H8 / SS0087

        Regular

        Mountain Grey

        RR23 / SS0036

        Regular

        Nordic Night Black

        RR33 / SS0015

        Regular

        Acorn Brown

        RR827 / SS0434

        Regular

        Cottage Red

        RR29 / SS0758

        Regular

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

            Contact Information