    General Product Description

    SSAB Domex 500LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. SSAB Domex 500LA offers consistent properties that assist modern, rapid production methods.

    Dimension Range

    SSAB Domex 500LA is available in thicknesses of 0.50-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Yield strength ReL
      (MPa)
      Tensile strength Rm
      (MPa)
      Elongation A80 1)
      (min %)
      Min. inner bending radius for a 90° bend
      (x t) 2)
      500 - 620 570 - 710 14 0.5
      Compare parameters

      Select one parameter to compare

      Comparison

        The mechanical properties are tested in the transversal direction.
        Bending properties for both longitudinal and transversal direction.

        1) When the thickness is less than or equal to 0.7 mm, the minimum value for elongation is reduced by 2 units.

        2) t = Sheet thickness.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Al
          (min %)
          Nb+Ti
          (max %)
          0.10 0.60 1.80 0.030 0.025 0.015 0.10
          Compare parameters

          Select one parameter to compare

          Comparison

            Tolerances

            SSAB Domex LA products are supplied with thickness, width and length tolerances in accordance to EN 10131. Narrower tolerances are available upon request.

            Delivery Conditions

            Cold Rolled.

            Fabrication and Other Recommendations

            For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

            Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

            Contact Information

            www.ssab.com/contact