SSAB Domex® 280LA

Download data sheet

General Product Description

SSAB Domex 280LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. SSAB Domex 280LA offers consistent properties that assist modern, rapid production methods.

Dimension Range

SSAB Domex 280LA is available in thicknesses of 0.40-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

Mechanical Properties

Yield strength ReL
(MPa)
Yield strength ReL
(MPa)
280 - 350
Tensile strength Rm
(MPa)
370 - 450
Elongation A80
(min %)
26
Min. inner bending radius for a 90° bend 1)
(x t)
0.0

The mechanical properties are tested in the transversal direction.
Bending properties for both longitudinal and transversal direction.

1) t = Sheet thickness.

Chemical Composition (ladle analysis)

C
(max %)
C
(max %)
0.10
Si
(max %)
0.040
Mn
(max %)
0.90
P
(max %)
0.030
S
(max %)
0.025
Al
(min %)
0.015
Nb+Ti
(max %)
0.10

Tolerances

SSAB Domex LA products are supplied with thickness, width and length tolerances in accordance to EN 10131. Narrower tolerances are available upon request.

Delivery Conditions

Cold Rolled.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Contact Information

www.ssab.com/contact 
Copyright 2026