GreenCoat Mica BT

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

     GreenCoat Mica BT color coated steel is available in an exclusive, glittery matt textured finish. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

    GreenCoat Mica BT color coated steel offers a high level of durability for profiled roof tiles and profiles with high aesthetic demands. GreenCoat Mica BT possesses good gloss retention and color fastness and provides good protection against corrosion (RC5 class). The reverse side of the sheet is painted with a two-layer grey backside coating.

    GreenCoat Mica BT complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Matt
      Gloss 5
      Minimum inner bending radius 1.5 x sheet thickness
      Scratch resistance 30 N
      UV radiation resistance RUV3
      Corrosion resistance 1) RC5
      Stain resistance Very good
      Highest operating temperature 100 °C
      Fire classification, EN 13501-1 A2 s1 d0
      Coating thickness, nominal (primer + top coat) 30 µm
      Coating structure Structured
      Steel designation 2) S280GD, S320GD, S350GD
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.50 mm
      Steel width 2) 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Matt
        5
        Technical Properties
        Minimum inner bending radius
        Matt
        1.5 x sheet thickness
        Technical Properties
        Scratch resistance
        Matt
        30 N
        Technical Properties
        UV radiation resistance
        Matt
        RUV3
        Technical Properties
        Corrosion resistance 1)
        Matt
        RC5
        Technical Properties
        Stain resistance
        Matt
        Very good
        Technical Properties
        Highest operating temperature
        Matt
        100 °C
        Technical Properties
        Fire classification, EN 13501-1
        Matt
        A2 s1 d0
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Matt
        30 µm
        Technical Properties
        Coating structure
        Matt
        Structured
        Technical Properties
        Steel designation 2)
        Matt
        S280GD, S320GD, S350GD
        Technical Properties
        Zinc coating
        Matt
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Matt
        0.50 mm
        Technical Properties
        Steel width 2)
        Matt
        1000 - 1500 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        11 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat Mica BT

        Goosewing Grey

        RR2H5 / SS0461

        Matt

        Mountain Grey

        RR23 / SS0036

        Matt

        Cliff Grey

        RR288 / SS0455

        Matt

        Slate Grey

        RR2H3 / SS0534

        Matt

        Nordic Night Black

        RR33 / SS0015

        Matt

        Walnut Brown

        RR32 / SS0387

        Matt

        Acorn Brown

        RR827 / SS0434

        Matt

        Cottage Red

        RR29 / SS0758

        Matt

        Brick Red

        RR7F2 / SS0742

        Matt

        Red Clay

        RR7G3 / SS0762

        Matt

        Silver Fir Green

        RR5J3 / SS0975

        Matt

        To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.