    General Product Description

    Extra-high-hardness armor with very good resistance against penetration.

    Armox® 600T is used as an add-on protection plate or where weight is critical. Armox® 600T is available in thicknesses between 4 and 20 mm with a guaranteed hardness range of 570‑640 HBW.

    Benefits of Armox® 600T include:

    • Market-leading steel protection
    • Superior workshop properties
    • Optimized solutions
    • Perfect hardness/toughness balance, for combined penetration and blast protection
    • Expertise in ballistic protection from SSAB

    Armox® 600T is not intended for further heat treatment.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Thickness
      (mmin)
      Hardness
      (HBW)
      4.0 - 20.00.157 - 0.787 570 - 640
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness
        (mmin)
        4.0 - 20.00.157 - 0.787
        Hardness
        (HBW)
        570 - 640

         

        Mechanical Testing

        Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.

        Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.

          

        Ultrasonic testing

        According to EN ISO 10 160 Class E3S3.

        Impact Properties

        Hide/Show specific columns Edit
        Select columns to display
          Thickness
          (mmin)
          Min impact energy for transversal testing,
          Charpy V 10x10 mm test specimen 1)
          4.0 - 20.00.157 - 0.787 12 J / -40 °C8 ft-lbs / -40 °F
          Compare parameters

          Select one parameter to compare

          Comparison

            Thickness
            (mmin)
            4.0 - 20.00.157 - 0.787
            Min impact energy for transversal testing,
            Charpy V 10x10 mm test specimen 1)
            12 J / -40 °C8 ft-lbs / -40 °F

            1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.

            Chemical Composition (ladle analysis)

            Hide/Show specific columns Edit
            Select columns to display
              C *)
              (max %)
              Si *)
              (max %)
              Mn*)
              (max %)
              P
              (max %)
              S
              (max %)
              Cr*)
              (max %)
              Ni*)
              (max %)
              Mo*)
              (max %)
              B*)
              (max %)
              0.47 0.70 1.00 0.010 0.003 1.5 3.0 0.70 0.005
              Compare parameters

              Select one parameter to compare

              Comparison

                The steel is grain-refined. *) Intentional alloying elements.

                Tolerances

                More details are given in SSAB´s brochure Armox® Guarantees or on www.ssab.com.

                Thickness

                Hide/Show specific columns Edit
                Select columns to display
                  Thickness
                  (mmin)
                  Tolerance
                  (mmin)
                  4.0 - 12.90.157 - 0.508 - 0.0 / + 0.6- 0.00 / + 0.031
                  13.0 - 19.90.512 - 0.783 - 0.0 / + 0.8- 0.00 / + 0.031
                  20.00.787 - 0.0 / + 1.0- 0.00 / + 0.039
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Thickness
                    (mmin)
                    4.0 - 12.90.157 - 0.508
                    Tolerance
                    (mmin)
                    - 0.0 / + 0.6- 0.00 / + 0.031
                    Thickness
                    (mmin)
                    13.0 - 19.90.512 - 0.783
                    Tolerance
                    (mmin)
                    - 0.0 / + 0.8- 0.00 / + 0.031
                    Thickness
                    (mmin)
                    20.00.787
                    Tolerance
                    (mmin)
                    - 0.0 / + 1.0- 0.00 / + 0.039

                    Length and Width

                    According to SSAB´s dimension program.

                    • Tolerances conform to EN 10029 or to SSAB´s standard after agreement.
                    • Dimensional tolerances for plate with mill edge according to special agreement. 

                    Shape

                    Tolerances according to EN 10029.

                    Flatness

                    Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).

                    Surface Properties

                    According to EN 10163-2 Class B Subclass 3.

                    Delivery Conditions

                    The delivery condition is QT (Quenched and Tempered).

                    Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.