Ferritic-Bainitic steel: stretch edge flangeability for cold-forming

Ferritic-Bainitic are multi-phased steels with high hole expansion ratios and good edge stretch capabilities. FB steels are suited for cold-formed and punched flanges when lightweighting automotive components such as wheels, cross members, and other structural parts.

What is the definition of FB steels?

Hot-rolled Ferrite-Bainite (FB) is comprised of very fine sized grains of ferrite and bainite. The ferrite delivers high elongation performance and the bainite contributes to FB’s good edge stretchability. 

Their minimal hardness differences between their phases adds to FB steel’s high hole expansion (HHE) performance and stretch flangeability, both key measures of local formability. Compared to high strength low alloy (HSLA) steels with similar strength levels, ferritic-bainitic steels have increased total elongation as well as a higher strain-hardening exponent (n-value).

FB steel properties

  • High local formability — good for cold-forming of edge flanges with punched holes
  • High hole expansion ratios
  • Strong fatigue performance relative to its tensile strength; good for automotive parts subject to vibration
  • Good weldability, including resistance spot welding and arc welding

Chassis applications for ferritic-bainitic steels

With a combination of good fatigue performance and formability, hot-rolled Docol FB steels can be found in many chassis applications.

  • Suspension parts, including upper and lower control arms
  • Wheels
  • Beams and cross members
  • Chassis

 

Ferrite bainite steel for automotive applications

Grades and mechanical properties for Docol® FB steels

Product Family

Docol 600FB

Product name
Docol HR440Y580T FB
Coating
UC, GI*
Dimensions
T: 2.00 - 4.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.157 in
W: Up to 62.99 in
Standards
VDA 239-100
Datasheet

*Available upon request.

Forming Docol® ferrite-bainite steels

  • Particular useful for auto parts with stretched flanged edges, FB is designed for cold-forming, drawing, stamping and punching.
  • Readily weldable, including resistant spot welding (RSW).
  • Good hole expansion performance, useful for folding, bending and through-hole extensions.
Cold forming ferrite bainite steel

Additional benefits from Docol® FB steels

  • Good fatigue properties for parts subject to vibration.
  • Grades are available to meet OEM-specific standards and certifications.
  • Global support and availability.

Are you looking for OEM-specific FB grades?

Docol® FB steel grades are supplied to VDA 239-100:2016 or OEM standards. Please contact our technical support for customized ferritic-bainitic grades for your specific automotive component.

Custom AHSS for automotive OEMs

The benefits of Docol® FB steel for each team member

Safety engineers: Use higher strength steel to increase performance in crash-related components.

Lightweighting engineers: Achieve weight reductions and crack-free stretched edges with a cold-worked high strength steel.

Production engineers: Use cold-forming operations to produce parts featuring stretched flanged edges with punched holes.

Buyers: Leverage an economically priced AHSS steel that uses your existing cold-forming equipment and techniques.

Sustainability officers: Right now, Docol® FB steels have the embedded-CO2 equivalence of recycled steel and, in 2026, will become available in fossil-free grades.

Future-proof your life cycle assessment
Lower your embedded CO2

Docol® Ferrite-Bainite steel is “future proofed.”

TRIAL MATERIAL STOCK

Get FB samples in multiple sizes

SSAB ships coils, sheets and custom lengths of any size, typically in 1 to 2 weeks. Get AHSS samples for both our commercially available grades, as well as our newest steels still in development.

FAQ

Other steel categories

High strength, low alloy (HSLA) steels for cost-effective automotive lightweighting

High strength, low alloy steels are a cost-effective choice for increasing strength-to-weight ratios when compared to conventional mild carbon steels. HSLA steels also have excellent bendability and weldability and can increase the strength and/or decrease the weight for a variety of body-in-white and chassis automotive components, including suspensions, beams, and subframes.

Read more

Complex phase (CP) steels for the highest hole expansion ratios

Complex phase steels have the highest — up to 75% — hole expansion ratios available from advanced high strength steels. Their high HER values provide excellent cold-forming properties for punched and stretched edges/flanges, as well as deep-drawn shapes. CP steels’ superior yield strengths are used for high crash-energy absorption, while their elevated UTS levels enable thinner walls for significant automobile weight reductions.

Read more

High edge (HE) ductility HSLA steel

High edge ductility HSLA steel with greatly improved local formability and high hole expansion ratios – ideal for challenging auto components with complex designs on sheared stretched edges.

Read more

Martensitic steel: excellent formability-to-strength ratio

Martensitic steel combines tensile strengths up to 1700 MPa with good ductility, making it highly efficient for both vehicle lightweighting and improved crash protection — especially in anti-intrusion zones.

Read more

Dual phase with high formability/ductility for crack-free cold deep drawing

Dual phase with high formability/ductility (DH) steels are TRIP-assisted, 3rd Generation automotive steels with high global and local formability and good resistance to edge cracking. DH steel have excellent energy-absorbing properties, included reserved ductility during crash impact. DH grades are ideal for complex geometries, including cold deep drawing. DH steel's FLDs and HERs are superior to DP steels, enabling scrap reduction and more streamlined stamping.

Read more

Dual phase (DP) steel: excellent ductility and energy absorption

Dual phase automotive steels have an excellent balance of ductility, high tensile strengths, easy cold formability, and very good crash energy-absorption. Its high early-stage strain hardening (n-value) makes DP steel resistant to local necking due to strain redistribution — providing highly uniform elongation. Dual phase steel’s low yield-to-tensile-strength ratio creates high global formability for deep-drawing and high-stretching capacities — all with good weldability.

Read more

Press hardening steels (PHS) for complex shapes

Press hardening steels have four major advantages: they can be formed into very complex shapes, their ultimate tensile strength ranges up to 2000 MPa (290 ksi), there is little or no springback, and, with tailored tempering, you can combine “full hard zones” and “soft zones” for multi-function crash performance within a single part.

Read more
Copyright 2026