GreenCoat Crown BT

Download data sheet

General Product Description

GreenCoat Crown BT color coated steel is available in regular and matt finishes and offers a good range of colors inspired by Nordic nature. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat Crown BT offers a high level of durability for modular roofs and profiled roof tiles as well as for lock form roofs. It can also be used in sandwich panels for faҫades and wall claddings as it will keep its good look over time and stand up well against corrosion (RC5 class). The structured surface helps to protect against mechanical wear and is easy to handle during manufacturing.

GreenCoat Crown BT color coated steel offers high gloss retention and color fastness. The matt coating delivers the highest level of color and gloss repeatability as well as a formability which makes the product a perfect choice for modular roofing applications.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Crown BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Color and gloss repeatability
Matt
Excellent level 1)
Regular
Normal good level
Technical Properties
Technical Properties
Gloss
Matt
10
Regular
40
Technical Properties
Technical Properties
Minimum inner bending radius
Matt
1.0 x sheet thickness
Regular
1.5 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Matt
25 N
Regular
25 N
Technical Properties
Technical Properties
UV radiation resistance
Matt
RUV3
Regular
RUV3
Technical Properties
Technical Properties
Corrosion resistance 2)
Matt
RC5
Regular
RC5
Technical Properties
Technical Properties
Stain resistance
Matt
Very good
Regular
Very good
Technical Properties
Technical Properties
Highest operating temperature
Matt
100 °C
Regular
100 °C
Technical Properties
Technical Properties
Fire classification, EN 13501-1
Matt
A2 s1 d0
Regular
A2 s1 d0
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Matt
26 µm
Regular
26 µm
Technical Properties
Technical Properties
Coating structure
Matt
Structured
Regular
Structured
Technical Properties
Technical Properties
Steel designation 3)
Matt
S280GD, S320GD
Regular
S280GD, S320GD
Technical Properties
Technical Properties
Zinc coating
Matt
275 g/m2
Regular
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 3)
Matt
0.45 mm
Regular
0.45 mm
Technical Properties
Technical Properties
Steel width 3)
Matt
1000 - 1300 mm
Regular
1000 - 1500 mm

1) Excellent color and gloss repeatability for GreenCoat Crown BT matt colors is valid for different SSAB production batches produced during a half-year.

2) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

3) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

Colors

Below are the main colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

Contact Information

www.ssab.com/contact 
Copyright 2026