    General Product Description

    SSAB’s toughest, ultra-hard protection plate.

    Armox® 620T is a new member of SSAB’s appliqué armor family. Armox® 620T is for use where component weight reduction is essential.

    It is available in thicknesses between 6 and 15 mm, and not intended for further heat treatment.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Thickness
      (mm)
      Hardness
      (HRC)
      6.0 - 15.0 55 - 60
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness
        (mm)
        6.0 - 15.0
        Hardness
        (HRC)
        55 - 60

         

        Mechanical Testing

        Rockwell hardness test EN ISO 6508-1. Each treatment individual.

        Ultrasonic testing

        According to EN ISO 10 160 Class E3S3.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          C *)
          (max %)
          Si *)
          (max %)
          Mn*)
          (max %)
          P
          (max %)
          S
          (max %)
          Cr*)
          (max %)
          Ni*)
          (max %)
          Mo*)
          (max %)
          B*)
          (max %)
          0.46 0.70 1.00 0.010 0.003 1.0 2.5 0.60 0.005
          Compare parameters

          Select one parameter to compare

          Comparison

            The steel is grain-refined. *) Intentional alloying elements.

            Tolerances

            More details are given in SSAB´s brochure Armox® Guarantees or on www.ssab.com.

            Thickness

            Hide/Show specific columns Edit
            Select columns to display
              Thickness
              (mm)
              Tolerance
              (mm)
              6.0 - 12.9 - 0.0 / + 0.6
              13.0 - 15.0 - 0.0 / + 0.8
              Compare parameters

              Select one parameter to compare

              Comparison

                Thickness
                (mm)
                6.0 - 12.9
                Tolerance
                (mm)
                - 0.0 / + 0.6
                Thickness
                (mm)
                13.0 - 15.0
                Tolerance
                (mm)
                - 0.0 / + 0.8

                Length and Width

                According to SSAB´s dimension program.

                • Tolerances conform to EN 10029 or to SSAB´s standard after agreement.
                • Dimensional tolerances for plate with mill edge according to special agreement. 

                Shape

                Tolerances according to EN 10029.

                Flatness

                Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).

                Surface Properties

                According to EN 10163-2 Class B Subclass 3.

                Delivery Conditions

                The delivery condition is Q (Quenched).

                Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.