HYBRIT®. A new revolutionary steelmaking technology.

With HYBRIT® technology, SSAB aims to be the first steel company in the world to bring fossil-free steel to the market and largely eliminate carbon dioxide emissions from its own operations. Together with our partners and customers, SSAB are building a fossil-free value chain – paving the way to a greener future.​

How SSAB replaces CO2 emissions with water

For thousands of years, steel has been made using coal to remove oxygen from iron ore, emitting vast amounts of CO2 in the process. But, SSAB has revolutionized the industry with HYBRIT® technology, using hydrogen instead of coal in the ore reduction process, and emitting water instead of CO2.

What is HYBRIT?

In 2016, SSAB, LKAB (Europe’s largest iron ore producer) and Vattenfall (one of Europe’s largest energy companies) joined forces to create HYBRIT – an initiative that endeavors to revolutionize steelmaking. Using HYBRIT® technology, SSAB aims to replace coking coal, traditionally needed for ore-based steelmaking, with fossil-free electricity and hydrogen. The result will be the world’s first fossil-free steelmaking technology, with virtually no carbon footprint. Our goal is to reduce Sweden’s CO2 emissions by 10% and Finland’s by 7%.

The journey towards fossil-free steel

Interview with Martin Pei

“We want to take this technology to a commercial scale, so we can be the first steel company to put fossil-free steel on the market.” Watch Martin Pei, SSAB’s CTO and originator of the initiative, to talk about the HYBRIT project.

A piece of the future

Episode 1: The HYBRIT initiative

Watch the video to learn more about the HYBRIT project and the journey towards Fossil-free steel.

A piece of the future

Episode 2: HYBRIT research

Watch the video to learn more about the HYBRIT project – from a shovel in the ground to a pilot plant.

A piece of the future

Episode 3: It starts in the mine

Watch the video to learn more about the HYBRIT project – We will change the future and the industry.

A piece of the future

Episode 4: Fossil-free electricity is the key

Watch the video to learn more about the HYBRIT project – Innovation needs to happen along the whole value chain.

A piece of the future

Episode 5: Addressing the root cause

Watch the video to learn more about the HYBRIT project – paving the way toward fossil-free industry future and steel products

A piece of the future

Episode 6: We have done it

Watch the video to learn more about the HYBRIT project – the production of world’s first fossil-free steel.

A joint venture

LKAB logotype

LKAB

LKAB is an international and high-tech mining and minerals group that mines and upgrades the unique iron ore of northern Sweden for the global steel market. Sustainability is core to our business and our ambition is to be one of the industry’s most innovative, resource-efficient and responsible companies.

Visit LKAB
Vattenfall logotype

Vattenfall

Vattenfall is a leading European energy company, which for more than 100 years has electrified industries, supplied energy to people’s homes and modernised our way of living through innovation and cooperation. We now want to make fossil-free living possible within one generation.

Visit Vattenfall
woman and child lying on the ground.

What does ”green steel” really mean?

The interest in “green steel” is increasing. But when no official definition exists, how do you know if you’re a victim of greenwashing?

Read more about green steel
download icon

Downloads

The place to go for corporate, financial, product or technical information.

To Download center
webinar icon

Webinars

Keep up-to-date on the latest product, design and manufacturing news.

Watch on demand or sign in
Social media icons

Follow us

Stay in touch with SSAB and our people, brands and customers in the channels you prefer.

See what’s on in each channel

Join us on the journey towards a fossil-free future

Contact us to find out more on how our steels can contribute to your sustainability goals and future growth. ​ ​

Country*
State/Region/Province*
Select product & brand*
What is your industry?*
Your function/role*

Please visit SSAB’s privacy statement for more information on how we process personal data.