Toolox® 40

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    The pre-hardened, exceptionally clean engineering and tool steel.

    Toolox® 40 is a pre-hardened steel suitable for engineering components and mold applications. It possesses good dimensional stability after machining.

    Toolox® 40 features the same machinability as the conventional P20/W.Nr 1.2311 steel, despite its nearly 100 HBW higher nominal hardness, in combination with the renowned high dimensional stability of Toolox®. This makes Toolox® 40 your ideal choice in engineering components that require higher strength, or in molds and dies that demand higher wear resistance.

    Dimension Range

    Toolox® 40 is available as plates in thicknesses between 6.0 - 130.0 mm. Other dimensions can be available on request.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Thickness
      (mm)
      Hardness 1)
      (HBW)
      6.0 - 130.0 360 - 420
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness
        (mm)
        6.0 - 130.0
        Hardness 1)
        (HBW)
        360 - 420

        1) Hardness is measured, according to EN ISO 6506-1, on a milled surface 0.5 - 2 mm below the plate surface.

        Impact Properties

        Hide/Show specific columns Edit
        Select columns to display
          Thickness
          (mm)
          Min impact energy for transversal testing,
          Charpy V 10x10 mm test specimen 1)
          6.0 - 130.0 20 J / 20 °C
          Compare parameters

          Select one parameter to compare

          Comparison

            Thickness
            (mm)
            6.0 - 130.0
            Min impact energy for transversal testing,
            Charpy V 10x10 mm test specimen 1)
            20 J / 20 °C

            1) Impact testing according to EN 10 025, EN ISO 148 with a 2 mm striker.

             

             

             

            Ultrasonic testing

            Ultrasonic inspection is carried out according to : EN 10 160 with extra demands according to specification SSAB V6.

            Tolerances

            More details are given in SSAB’s brochure Toolox® Guarantees and on www.toolox.com.

            Thickness

            Tolerances according to Toolox® Thickness Guarantee.

            Toolox® Guarantees meets the requirements of EN 10029 Class C but offers more narrow tolerances.

            Length and Width

            Tolerances according to EN 10029.

            Flatness

            Tolerances are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).

            Surface Properties

            According to EN 10163-2 Class B Subclass 3.

            Delivery Conditions

            Quenched and Tempered at a minimum temperature of 590 °C.

            On delivery from SSAB the plates meet the following specifications:

            • Free from mill scale
            • Not repair welded

            Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.toolox.com.