General Product Description

SSAB Domex 350LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. SSAB Domex 350LA offers consistent properties that assist modern, rapid production methods.

Dimension Range

SSAB Domex 350LA is available in thicknesses of 0.45-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Yield strength ReL
    (MPa)
    Tensile strength Rm
    (MPa)
    Elongation A80 1)
    (min %)
    Min. inner bending radius for a 90° bend
    (x t) 2)
    350 - 440 410 - 530 22 0.0
    Compare parameters

    Select one parameter to compare

    Comparison

      The mechanical properties are tested in the transversal direction.
      Bending properties for both longitudinal and transversal direction.

      1) When the thickness is less than or equal to 0.7 mm, the minimum value for elongation is reduced by 2 units.

      2) t = Sheet thickness.

      Chemical Composition (ladle analysis)

      Hide/Show specific columns Edit
      Select columns to display
        C
        (max %)
        Si
        (max %)
        Mn
        (max %)
        P
        (max %)
        S
        (max %)
        Al
        (min %)
        Nb+Ti
        (max %)
        0.10 0.040 0.90 0.030 0.025 0.015 0.10
        Compare parameters

        Select one parameter to compare

        Comparison

          Tolerances

          SSAB Domex LA products are supplied with thickness, width and length tolerances in accordance to EN 10131. Narrower tolerances are available upon request.

          Delivery Conditions

          Cold Rolled.

          Fabrication and Other Recommendations

          For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

          Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

          Contact Information

          www.ssab.com/contact