Nombre del producto | Dimensiones | Dureza | Estándares | Ficha técnica |
---|---|---|---|---|
Armox® 370T Class 1 | T: 3.0 - 100.0 mm | 300 - 430 HBW | EN 10029 | |
Armox® 370T Class 2 | T: 3.0 - 100.0 mm | 280 - 330 HBW | EN 10029 | |
Armox® 440T | T: 4.0 - 80.0 mm | 420 - 480 HBW | EN 10029 | |
Armox® 500T | T: 3.0 - 80.0 mm | 480 - 540 HBW | EN 10029 | |
Armox® 520T | T: 4.0 - 12.0 mm | 500 - 550 HBW | EN 10029 | |
Armox® 560T | T: 4.0 - 15.0 mm | 530 - 590 HBW | EN 10029 | |
Armox® 600T | T: 4.0 - 20.0 mm | 570 - 640 HBW | EN 10029 | |
Armox® 620T | T: 6.0 - 15.0 mm | 55 - 60 HRC | EN 10029 | |
Armox® Advance | T: 4.0 - 7.9 mm | 58 - 63 HRC | EN 10029 |
Nombre del producto | Dimensiones | Dureza | Estándares | Ficha técnica |
---|---|---|---|---|
Ramor® 450 | T: 8.00 - 16.00 mm | 400 - 480 HBW | EN 10029 | |
Ramor® 500 | T: 2.0 - 30.0 mm | 490 - 560 HBW | EN 10029, EN 10051 | |
Ramor® 550 | T: 3.0 - 15.0 mm | 540 - 600 HBW | EN 10029, EN 10051 | |
Ramor® 600 | T: 3.0 - 6.0 mm | 570 - 640 HBW | EN 10051 |