American Bureau of Shipping/ABS Steel Grades

Many of our SSAB facilities carry and maintain ABS certifications to  supply ordinary-strength to high-strength steels with improved toughness and Reduction of Area. Our ABS grades are used in the Ship Building(Marine) and mobile offshore drilling units and structures.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.1875 - 5.9 Inches

W: Up to 130 Inches

L: Up to 1020 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.185 - 5.9 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.185 - 4 Inches

W: Up to 130 Inches

L: Up to 600 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.1875 - 1.57 Inches

W: Up to 130 Inches

L: Up to 1020 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.315 - 2.56 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ABS Grade EQ47
USED FOR

Structural

DIMENSIONS

T: 0.472 - 1.57 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ABS Grade EQ51
USED FOR

Structural

DIMENSIONS

T: 0.393 - 1.57 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ABS AQ/DQ/EQ 63
USED FOR

Structural

DIMENSIONS

T: 0.188 - 1.5 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English

PRODUCT NAME
ABS AQ/DQ/EQ 70
USED FOR

Structural

DIMENSIONS

T: 0.188 - 1.5 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.1875 - 5.9 Inches

W: Up to 130 Inches

L: Up to 1020 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.157 - 5.9 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.157 - 4 Inches

W: Up to 130 Inches

L: Up to 600 Inches

DATA SHEET

English

PRODUCT NAME
ABS Grade A, B, D, E
USED FOR

Structural

DIMENSIONS

T: 0.1875 - 5.9 Inches

W: Up to 130 Inches

L: Up to 1020 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.6 - 5.9 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

USED FOR

Structural

DIMENSIONS

T: 0.185 - 4 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English