    In addition to SSAB producing coils to the ASTM 1011 and ASTM 1018 specifications, SSAB also produces as-rolled coils that can be converted by a coil processor to the requirements of the ASTM and CSA structural specifications, to ASTM pressure vessel steel specifications, and SSAB's Proprietary specifications. Inquire for other specifications and grades not listed in the table below, for example, API grades. SSAB will only certifythe as-rolled coils to the chemistry requirements of the respective specification.

    Dimension Range

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      A36 Coil for Conversion to 0.188 - 0.6254.78 - 15.9 60 - 961500 - 2400
      A242 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 60 - 961500 - 2400
      A283 Grades C and D Coil for Conversion to 0.188 - 0.6254.78 - 15.9 60 - 961500 - 2400
      A516 Grade 60, 65, and 70 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 72 - 961800 - 2400
      A572 Grade 42, 50, 55, and 60 Coil for Conversion to 0.188 - 0.6254.78 - 15.9 60 - 961500 - 2400
      A572 Grade 65 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 60 - 961500 - 2400
      A656 Grade 50 Coil for Conversion to 0.188 - 0.6254.78 - 15.9 60 - 961500 - 2400
      A656 Grades 60, 70, and 80 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 60 - 961500 - 2400
      A871 Grades 60 and 65 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 72 - 961800 - 2400
      AR200 Coil for Conversion to 0.188 - 0.5004.78 - 12.7 60 - 961500 - 2400
      AR235 Coil for Conversion to 0.188 - 0.3754.78 - 9.52 60 - 961500 - 2400
      CSA 38W, 38WT, 44W, 44WT, 50W and 50WT Coil for Conversion to 0.188 - 0.7504.78 - 19.0 60 - 961500 - 2400
      CSA 50A and 50AT Coil for Conversion to 0.188 - 0.5004.78 - 12.7 60 - 961500 - 2400
      CSA 60W and 60WT Coil for Conversion to 0.188 - 0.6254.78 - 15.9 60 - 961500 - 2400
      Compare parameters

      Select one parameter to compare

      Comparison

        Product Type: Coils are excluded from the qualification to the referenced plate specification until the coils are processed into a finished plate product and all required processing, inspections and testing are performed according to the respective specification. SSAB will certifythe as-rolled coils to the chemistry requirements only. Any tensile testing information provided by SSAB shall not be used for certifying any cut-to-length sheets to the governing specifications.

        Thickness: Please inquire for thicknesses less than or greater than the specified minimums or maximums.

        Width: Please inquire for widths less than or greater than the noted minimums or maximums.