Toolox® 46

Pre-hardened, precise, predictable steel, now available as plate, forged block and as round bars

Download data sheet

General Product Description

Toolox® 46 is a steel delivered already heat treated to a very high hardness.

The chemical composition is based on the succesful Toolox® 44 product but with a modified chemical composition making this a perfect choice for the most demanding hot work tooling applications. Despite the high hardness, machining can be carried out smoothly with normal carbide tooling. If necessary the surface properties can be further enhanced with nitriding, laser and PVD.

Dimension Range

Toolox® 46 is available as plates in thicknesses between 2.362" - 5.118", as forged block in thicknesses between 6.693" - 12.598", and as round bars in diameters between 5.945" - 13.898". Other dimensions can be available on request. For more information concerning dimensions and tolerances, see Toolox® round bars or Toolox engineering & tool steel dimensional program

Mechanical Properties

Product
Product
Plate
Thickness
(inmm)
2.362 - 5.11860.0 - 130.0
Diameter (inmm)
—
Hardness 1)
(HBW)
430 - 490
Product
Product
Forged block
Thickness
(inmm)
6.693 - 12.598170.0 - 320.0
Diameter (inmm)
—
Hardness 1)
(HBW)
430 - 490
Product
Product
Round bar
Thickness
(inmm)
—
Diameter (inmm)
5.945 - 13.898151.0 - 353.0
Hardness 1)
(HBW)
430 - 490

1) Hardness is measured, according to EN ISO 6506-1. The measurement is performed on a milled surface 0.492" below the ordered surface for forged blocks and round bars. Bar hardness is measured with indents positioned as impact test according to EN 10083. For plate the measurment is preformed on a milled surface 0.020" - 0.079" below the surface.

 

 

Impact Properties

Product
Product
Plate
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
6 ft-lbs / 68 °F8 J / 20 °C
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
—
Product
Product
Forged block
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
8 ft-lbs / 68 °F11 J / 20 °C
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
—
Product
Product
Round bar
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
—
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
8 ft-lbs / 68 °F11 J / 20 °C

1) Impact testing according to EN 10 025, EN ISO 148 with a 0.079" striker.

2) Impact testing according to EN 10083.

Ultrasonic testing

Ultrasonic inspection is carried out according to: EN 10160 for plate, EN 10228-3 for forged blocks and EN 10308 for round bars . All of them with extra demands according to specification SSAB V6.

Tolerances

For more information concerning dimensions and tolerances, see Toolox® dimensional programs or Toolox® Guarantees available at www.ssab.com or www.toolox.com.

Thickness

Tolerances according to Toolox® Thickness Guarantee.

Toolox® Guarantees meets the requirements of EN 10029 Class C, but offers more narrow tolerances for plates.

Thickness tolerances for Toolox® forged blocks are according to 0"/+0.126".

Bar Diameter

Tolerances according to EN 10060.

Length and Width

Length and width tolerances according to EN 10029 for Toolox® plates.

Length tolerances for Toolox® forged blocks are -9.685"/+9.685".

Length tolerances for Toolox® round bar are according to EN 10060 with tolerances -0/+7.874".

Flatness

Tolerances for Toolox® plates are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).

Maximum accepted flatness deviation for Toolox® forged blocks are 0.039"/39.370".

Bar Straightness

Tolerances according to EN 10060, with a maximum allowed deviation of 0.079".

Surface Properties

According to EN 10163-2 Class B, Subclass 3 for Toolox® plate.

Surface condition for Toolox® forged blocks is machined surface plus oiling.

Surface condition for Toolox® round bars are turned and oiled.

Delivery Conditions

Quenched and Tempered at a minimum temperature of 1094 °F.

On delivery from SSAB, Toolox® material meet the following specifications:

 

  • Free from mill scale
  • Not repair welded

 

Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.ssab.com.

Recommendations and instructions

Used for

  • Tooling & Engineering
  • High temperatures (up to 590°C)

Available standard

  • EN10060

High-strength engineering tool steel

The new generation of tool steel.