    ABS Grades AH32, DH32, and EH32 are higher-strength structural steels with a minimum specified yield strength of 46 ksi and specified minimum Charpy V- notch impact toughness properties.

    Applications

    Typical applications include shipbuilding and mobile offshore drilling units and structures.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inmm)
      Width
      (inmm)
      Length
      (inmm)
      Grade AH32 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Grade DH32 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Grade EH32 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Please inquire for plate widths less than 72 in. and inquire plate product over 120 in.

        Length: Please inquire for plate lengths less than 240 in. and greater than the listed maximum.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (inmm)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation A5 1)
          (min %)
          Grade AH32 0.1875 - 5.904.762 - 150 46 64 - 85 22
          Grade DH32 0.1875 - 5.904.762 - 150 46 64 - 85 22
          Grade EH32 0.1875 - 5.904.762 - 150 46 64 - 85 22
          Compare parameters

          Select one parameter to compare

          Comparison

            1) See ABS Rules for elongation requirements for alternative tensile specimens.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Grade Thickness
              (inmm)
              Test temperature
              (°F)
              Min Longitudinal Average Energy 1)
              (ft-lbs)
              Min transverse average energy 1)
              (ft-lbs)
              AH32 0.1875 - 2.004.762 - 50.8 32 23 16
              AH32 2.001 - 2.8050.83 - 71.1 32 28 19
              AH32 2.801 - 5.9071.15 - 150 32 34 23
              DH32 0.1875 - 2.004.762 - 50.8 -4 23 16
              DH32 2.001 - 2.8050.83 - 71.1 -4 28 19
              DH32 2.801 - 5.9071.15 - 150 -4 34 23
              EH32 0.1875 - 2.004.762 - 50.8 -40 23 16
              EH32 2.001 - 2.8050.83 - 71.1 -40 28 19
              EH32 2.801 - 5.9071.15 - 150 -40 34 23
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Specimen orientation at the option of the manufacturer unless otherwise specified in the order.

                No more than one value below the specified miniminum average energy but no less than 70% of the specfied minimum average energy value.

                Minimum average energy for full-size specimens. Refer to ABS Rules for sub-size specimen energy requirements.

                Carbon Equivalent

                Hide/Show specific columns Edit
                Select columns to display
                  Grade AH32 AH32 DH32 DH32 EH32 EH32
                  Thickness (inmm) 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2
                  CEV 1) (max %) 0.36 0.38 0.36 0.38 0.36 0.38