Combines ballistic properties with impact toughness.

 

Ramor® 450 is a medium-hard protection plate combining ballistic properties with impact toughness, at 8.0 ‑ 16.0 mm (0.315‑0.630″) thick and 400‑480 HBW. Ramor® 450 is not intended for further heat treatment.

 

Mechanical Properties

Ramor® 450

Thickness
(inmm)
0.315 - 0.6308.00 - 16.00
Hardness
(HBW)
400 - 480
Yield strength Rp0.2
(min ksiMPa)
1451000
Tensile strength Rm
(min ksiMPa)
1671150
Elongation A5
(min %)
8

Mechanical Testing

Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.

Hardness is measured on a milled surface 0.012 - 0.079" below plate surface.  

Charpy impact test according to EN ISO 148, 1 test/20 ton. 

Tensile test according to EN ISO 6892 on each plate and thickness <0.783".

Impact Properties

Thickness
(inmm)
Thickness
(inmm)
0.315 - 0.6308.00 - 16.00
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
15 ft-lbs / -40 °F20 J / -40 °C

1) Impact testing transverse to rolling direction, average value of three tests. Single value min. 70% of specified average.

 

 

Chemical Composition (heat analysis)

C
(max %)
C
(max %)
0.25
Si
(max %)
0.70
Mn
(max %)
1.50
P
(max %)
0.015
S
(max %)
0.010
Cr
(max %)
1.00
Ni
(max %)
2.0
Mo
(max %)
0.70
B
(max %)
0.005

The steel is grain-refined. Phosphorous and sulphur are not intentionally alloying elements.

Tolerances

More details are given on www.ssab.com.

Thickness

Product Type
Product Type
Plate
Thickness
(inmm)
0.315 - 0.5878.00 - 14.9
Tolerance
(inmm)
- 0.0 / + 0.0394- 0.0 / + 1.0
Product Type
Product Type
Plate
Thickness
(inmm)
0.590 - 0.63015.0 - 16.0
Tolerance
(inmm)
- 0.0 / + 0.0433- 0.0 / + 1.1

Length and Width

Tolerances conform to EN 10029 or to SSAB´s standard after agreement.

Dimensional tolerances for plate with mill edge according to special agreement. 

Shape

Tolerances according to EN 10029.

Flatness

Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10029 Class N (steel type L).

Surface Properties

According to EN 10163-2 Class B Subclass 3.

Delivery Conditions

Ramor® is delivered in quenched condition.