Strenx® 1100 product group

Strenx® 1100 is a group of structural steel grades with a minimum yield strength of 1100 MPa (160 ksi). Excellent for advanced lifting devices.

SUITABLE APPLICATIONS
Advanced lifting devices and lighter transport solutions

TYPE OF PRODUCTS
Hot rolled strip, Plate, Cold rolled strip

THICKNESS RANGE
0,8 - 40 mm (0.031’’ – 1.57’’)

A wide range of high-strength structural steels for high-performing applications

STRENX® 1100 E
Superior toughness

Made for advanced lifting devices, such as mobile cranes, and lighter transport solutions and components

Impact toughness: 27 J/-40°C (20 ft-lb/-40°F)
Plate: 4-40 mm (0.157’’ – 1.57’’)
Standard: SSAB specification
Format: Plate

Go to Strenx® 1100 E/F

STRENX® 1100 F
Extreme toughness

Made for advanced lifting devices, such as mobile cranes, and lighter transport solutions and components in cold conditions

Impact toughness: 27 J/-60°C (20 ft-lb/-76°F)
Plate: 4-40 mm (0.157’’ – 1.57’’)
Standard: SSAB specification
Format: Plate

Go to Strenx® 1100 E/F

STRENX® 1100MC
Multipurpose cut-to-length sheets

Load-bearing structures, where strength and weight is critical

Impact toughness: 27 J/-40°C (20 ft-lb/-40°F)
Hot rolled strip: 3-8 mm (0.118’’ – 0.393’’)
Standard: SSAB specification
Format: Sheet

Go to Strenx® 1100 MC

STRENX® 1100 CR
For the thinnest structural parts

A wide range of components and parts in the lightest possible load-bearing structures

Cold rolled strip: 0.8-2.1 mm (0.032’’ –0.082”)
Standard: SSAB specification
Format: Sheet

Go to Strenx® 1100 CR
Upgrade your design

Upgrade your design – reach new heights

Mobile cranes, loader cranes, work platforms and other lifting equipment can achieve new levels of performance by using Strenx® 1100 high-strength structural steel. Optimizing the design to take advantage of the high strength makes the equipment lighter, giving increased load capacity and longer reach. For support on designing with Strenx® 1100, get in touch with SSAB Tech Support.

Contact tech support

Made for predictable performance in the workshop

Person welding Strenx® high-strength steel in the workshop.

Welding

Strenx® 1100 can be welded using any conventional welding method. MAG welding is the most common technique today, since it is very easy to automate for high productivity.

Machining

Strenx® 1100 can usually be machined without special equipment. Stable machinery fitted with high-speed steel and carbide tools is recommended when drilling, countersinking, tapping, turning, and milling.

Bending

Free bending and roll bending of Strenx® steel plate and strip can be done using standard bending machinery. Uniform properties, close thickness tolerances and high surface quality ensure a predictable bending process.

Thermal cutting

The properties and fine surface finish of Strenx®1100 plate and strip makes it perfect for laser cutting. Thermal cutting of hot-rolled Strenx® 1100 steel sheet and plate is performed with oxy-fuel flame, plasma and laser.

Mechanical cutting

Mechanical cutting of Strenx® 1100 is best performed with guillotine shears. Consider carefully the settings of the cutting machine. The most important factors are clearance, cutting angle and blade hardness. The plate should be allowed to warm up thoroughly to around +20°C before it is cut.

Strenx® guarantees

Strenx® guarantees include tight thickness tolerances, tight flatness tolerances and bending guarantees. The tight thickness tolerances enable you to know the weight more precisely. As a result, you can reduce your safety margins. Precise thickness within a plate and between plates makes for safe and predictable performance in the workshop.

LEARN MORE ABOUT YOUR GUARANTEES

Strenx® performance steel has the right strength for the world’s No. 1 crawler crane, the XCMG’s 4000-ton

Tension bars in Strenx® 1100 E a safe choice in XCMG’s record-breaking crawler cranes.

Read the full story
Strenx® 1100
standard products
Thickness range [mm]Confirm to standardFormatsTypical products manufactured with Strenx®
PlateHot rolled stripCold rolled strip
Strenx® 1100 E4-40------SSAB specificationPlatesAdvanced lifting devices, such as mobile cranes, and lighter transport solutions and components
Strenx® 1100 F4-40------SSAB specificationPlatesAdvanced lifting devices, such as mobile cranes, and lighter transport solutions and components
in cold conditions
Strenx® 1100 MC---3-8---SSAB specificationSheetsLoad-bearing structures, where strength and weight is critical
Strenx® 1100 CR------0.8-2.1SSAB specificationSheets & CoilsA wide range of components and parts in the lightest possible load-bearing structures
Copyright 2026