Your guide to Strenx® structural steel

High-strength Strenx® structural steel makes your products stronger, lighter, safer, more competitive and more sustainable. Find out how segments like transportation, lifting, agriculture and others are gaining the benefits. Explore our wide range of Strenx® products, from plate, sheet and coil to tubes and sections.

Show specs in:

ImperialMetric

Local stocks or mill-direct, wherever and whenever you need it

Get Strenx® delivered through a reliable supply chain and advanced logistics services – wherever you are in the world, whenever you need it, and in the agreed condition. SSAB offers local stocks worldwide, mill-direct deliveries, value-added processing and logistics management solutions. 

Find your local stocks

Comprehensive technical support at your fingertips

As a Strenx® structural steel customer, you gain full access to a wide variety of services that go above and beyond traditional support. You can get technical support in the most common languages in the world, from design and development support to workshop fabrication recommendations, as well as expert advice, technical training and tools that can make you more productive – and take your business to new heights.  

Contact our support team

Strenx® 700

Strenx® 700 is a group of structural steels with a minimum yield strengths between 650 and 700 MPa (94-101 ksi) depending on thickness.

Product Name

Strenx® 700 CR

Thickness range (inmm)
0.03 - 0.0830.7 - 2.1
Yield strength (min ksiMPa)
101700
Standards
SSAB Specification
Datasheet
Product Name

Strenx® 700 E/F

Thickness range (inmm)
0.157 - 6.2994.0 - 160.0
Yield strength (min ksiMPa)
94 - 101650 - 700
Standards
EN 10025-6
Datasheet
Product Name

Strenx® 700 OME

Thickness range (inmm)
0.157 - 5.1184.0 - 130.0
Yield strength (min ksiMPa)
101700
Standards
EN 10025-6
Datasheet
Product Name

Strenx® 700MC D/E

Thickness range (inmm)
0.079 - 0.3932.00 - 10.00
Yield strength (min ksiMPa)
101700
Standards
EN 10149-2
Datasheet
Product Name

Strenx® 700MC Plus

Thickness range (inmm)
0.118 - 0.4723.0 - 12.0
Yield strength (min ksiMPa)
101700
Standards
EN 10149-2
Datasheet
Product Name

Strenx® P700

Thickness range (inmm)
0.157 - 3.9374.0 - 100.0
Yield strength (min ksiMPa)
97 - 101670 - 700
Standards
EN 10028-6
Datasheet
Product Name

Strenx® 700 CR W

Thickness range (inmm)
0.03 - 0.0830.7 - 2.1
Yield strength (min ksiMPa)
700
Standards
-
Datasheet
Product Name

Strenx® 700 HR W

Thickness range (inmm)
0.118 - 0.3153.0 - 8.0
Yield strength (min ksiMPa)
101700
Standards
EN 10149-2
Datasheet

Strenx® 900

Strenx® 900 is a group of high-strength structural steel grades with a minimum yield strengths between 830 and 900 MPa (120 - 130 ksi), making them an excellent choice for transportation and lifting devices.

Product Name

Strenx® 900 E/F

Thickness range (inmm)
0.157 - 4.7244.0 - 120.0
Yield strength (min ksiMPa)
120 - 130830 - 900
Standards
EN 10025-6
Datasheet
Product Name

Strenx® 900MC

Thickness range (inmm)
0.118 - 0.3933.00 - 10.00
Yield strength (min ksiMPa)
130900
Standards
EN 10149-2
Datasheet
Product Name

Strenx® 900 Plus

Thickness range (inmm)
0.079 - 0.3152.0 - 8.0
Yield strength (min ksiMPa)
130900
Standards
EN 10025-6
Datasheet

Strenx® 960

Strenx® 960 is a group of high-strength structural steel grades with a minimum yield strengths between 850 of 960 MPa (123-139 ksi), making them an excellent choice for transportation and lifting devices.

Product Name

Strenx® 960 E/F

Thickness range (inmm)
0.157 - 4.7244.0 - 120.0
Yield strength (min ksiMPa)
123 - 139850 - 960
Standards
EN 10025-6
Datasheet
Product Name

Strenx® 960MC

Thickness range (inmm)
0.118 - 0.3933.00 - 10.00
Yield strength (min ksiMPa)
139960
Standards
EN 10149-2
Datasheet
Product Name

Strenx® 960 Plus

Thickness range (inmm)
0.079 - 0.3152.00 - 8.00
Yield strength (min ksiMPa)
139960
Standards
EN 10025-6
Datasheet
Product Name

Strenx® 960 CR

Thickness range (inmm)
0.03 - 0.0830.8 - 2.1
Yield strength (min ksiMPa)
139960
Standards
SSAB Specification
Datasheet
Product Name

Strenx® 960 HR W

Thickness range (inmm)
0.118 - 0.2403.0 - 6.1
Yield strength (min ksiMPa)
139960
Standards
EN 10149-2
Datasheet

Strenx® 1100

Strenx® 1100 is a group of structural steel grades with a minimum yield strength of 1100 MPa (160 ksi). Excellent for advanced lifting devices.

Product Name

Strenx® 1100 E/F

Thickness range (inmm)
0.157 - 1.5754.0 - 40.0
Yield strength (min ksiMPa)
1601100
Standards
SSAB Specification
Datasheet
Product Name

Strenx® 1100MC

Thickness range (inmm)
0.118 - 0.3153.00 - 8.00
Yield strength (min ksiMPa)
1601100
Standards
SSAB Specification
Datasheet
Product Name

Strenx® 1100 CR

Thickness range (inmm)
0.03 - 0.0830.8 - 2.1
Yield strength (min ksiMPa)
1601100
Standards
SSAB Specification
Datasheet

Strenx® 1300

Strenx® 1300 is a group of structural steel grades with a minimum yield strength of 1300 MPa (188 ksi). Excellent for advanced lifting devices.

Product Name

Strenx® 1300 E/F

Thickness range (inmm)
0.157 - 0.5914.0 - 15.0
Yield strength (min ksiMPa)
1881300
Standards
SSAB Specification
Datasheet

Strenx® 100/110

The high-strength, high-performance steel with a minimum yield strength of 100 ksi.

Product Name

Strenx® 100

Thickness range (in)
0.188 - 5.000
Yield strength (min ksi)
94 - 100
Standards
ASTM A514
Datasheet
Product Name

Strenx® 100 XF

Thickness range (in)
0.079 - 0.393
Yield strength (min ksi)
100
Standards
SSAB Specification
Datasheet
Product Name

Strenx® 110 XF

Thickness range (in)
0.079 - 0.393
Yield strength (min ksi)
110
Standards
ASTM A1011 or A1018 on request
Datasheet

Strenx® weathering

Strenx® weathering grades will give your high-strength steel applications additional protection against corrosion.

Product Name

Strenx® 700 CR W

Thickness range (inmm)
0.03 - 0.0830.7 - 2.1
Yield strength (min MPa)
700
Standards
-
Datasheet
Product Name

Strenx 700HR W

Thickness range (inmm)
0.118 - 0.3153.0 - 8.0
Yield strength (min MPa)
101700
Standards
EN 10149-2
Datasheet
Product Name

Strenx 960HR W

Thickness range (inmm)
0.118 - 0.2403.0 - 6.1
Yield strength (min MPa)
139960
Standards
EN 10149-2
Datasheet

Strenx® Tubes

Strenx® Tubes are tubes that combine high strength with a naturally stiff welded hollow section, enabling you to build stronger and lighter structures.

Product Name

Strenx® Tube 700MLH

Shapes
Circular, Rectangular, Square
Thickness range (inmm)
0.098 - 0.3932.5 - 10.0
Circular (inmm)
1.669 - 12.75248.3 - 323.9
Square (inmm)
1.575x1.575 - 11.811x11.81140x40 - 300x300
Rectangular (inmm)
1.969x1.181 - 15.748x7.87450x30 - 400x200
Yield strength (min ksiMPa)
101700
Standards
EN 10219-3
Datasheet
Product Name

Strenx® Tube 900MH

Shapes
Circular, Rectangular, Square
Thickness range (inmm)
0.157 - 0.2364.0 - 6.0
Circular (inmm)
5.500 - 8.626139.7 - 219.1
Square (inmm)
3.937x3.937 - 7.874x7.874100x100 - 200x200
Rectangular (inmm)
4.724x3.149 - 9.843x5.906120x80 - 250x150
Yield strength (min ksiMPa)
130900
Standards
EN 10219-3
Datasheet
Product Name

Strenx® Tube 960MH

Shapes
Circular, Rectangular, Square
Thickness range (inmm)
0.157 - 0.2364.0 - 6.0
Circular (inmm)
5.500 - 8.626139.7 - 219.1
Square (inmm)
3.937x3.937 - 7.874x7.874100x100 - 200x200
Rectangular (inmm)
4.724x3.149 - 9.843x5.906120x80 - 250x150
Yield strength (min ksiMPa)
139960
Standards
EN 10219-3
Datasheet
Product Name

Strenx® Tube 960QLH

Shapes
Circular
Thickness range (inmm)
0.118 - 0.2363.0 - 6.0
Circular (inmm)
3.000 - 5.23676.1 - 133.0
Square (inmm)
-
Rectangular (inmm)
-
Yield strength (min ksiMPa)
140960
Standards
EN 10210
Datasheet

Strenx® Sections

Strenx® Sections are cold-formed steel section made of hot-rolled, high-strength steel.

Product Name

Strenx® Section 650MC

Thickness range (inmm)
0.098 - 0.3142.5 - 8.0
Yield strength (min ksiMPa)
94650
Standards
EN 10162
Datasheet
Product Name

Strenx® Section 700MC

Thickness range (inmm)
0.098 - 0.3142.5 - 8.0
Yield strength (min ksiMPa)
101700
Standards
EN 10162
Datasheet
Product Name

Strenx® Section 900MC

Thickness range (inmm)
0.118 - 0.2363.0 - 6.0
Yield strength (min ksiMPa)
130900
Standards
EN 10162
Datasheet

Strenx® 600

The high-strength structural steel at 600 MPa.

Product Name

Strenx® 600MC D/E

Thickness range (inmm)
0.079 - 0.3932.00 - 10.00
Yield strength (min ksiMPa)
87600
Standards
EN 10149-2
Datasheet

Strenx® 650

The high-strength structural steel at 650 MPa.

Product Name

Strenx® 650MC D/E

Thickness range (inmm)
0.079 - 0.3932.00 - 10.00
Yield strength (min ksiMPa)
94650
Standards
EN 10149-2
Datasheet