Strenx® 1300 E/F is an ultra-high-strength structural steel with a minimum yield strength of 188 ksi.
Typical applications include load-carrying structures that place very high demands on low weight. SSAB developed Strenx® 1300 E/F for building the lightest possible steel solutions or providing an alternative to other materials.
Strenx® 1300 E/F benefits include:
For transverse test pieces.
The steel is grain refined. *) Intentional alloying elements.
Strenx® 1300 E
Strenx® 1300 F
Tolerances according to Strenx® Thickness Guarantees.
Strenx® Guarantees meet the requirements of EN 10029 Class A, but offers narrower tolerances.
According to SSAB’s dimension program. Tolerances conforms with EN 10029.
Tolerances according to EN 10029.
Tolerances according to Strenx® Flatness Guarantee Class D, which are more narrow than EN 10029 Class N.
According to EN 10163-2 Class A, Subclass 3.
The delivery condition is Quenched and Tempered. The plates are delivered with sheared or thermally cut edges. Untrimmed edges after agreement.
Delivery requirements can be found in SSAB’s brochure Strenx® Guarantees or on www.ssab.com.
Recommendations are found in SSAB’s brochures at www.ssab.com or consult Tech Support.
Bendability according to Strenx® Bending Guarantee.
Strenx® 1300 E/F has obtained its mechanical properties by quenching and subsequent tempering. The properties of the delivery condition cannot be retained after exposure to temperatures in excess of 392ºF.
Appropriate health and safety precautions must be taken when welding, cutting, grinding or otherwise working on this product. Grinding, especially of primer coated plates, may produce dust with a high particle concentration.