Processing services – Take advantage of our tailored steel services

By combining our premium steel products and experience with engineering support and prefabrication, you get a service that is hard to match. So, let us do the preprocessing. You will save on time and paperwork, reduce tied up inventory and, in the end, achieve a more innovative and competitive end product.

Adding value to the final product

SSAB provides services that include product delivery, technical support, and conceptual designs. We also offer amenities from processing services and workshop solutions, to innovation services and ready-made kits and components (with all the necessary assembly instructions).

SSAB can offer the following steel processing services:

Laser cutting

Max thickness 20 mm.
Max length 35,000 mm.

Find out more

Plasma cutting

Max thickness 50 mm.
Max length 37,000 mm.

Flame cutting

Max thickness 380 mm.
Max length 37,000 mm.

Find out more

Laser welding

Max length 20,000 mm.
Max thickness 8 mm.

Find out more

Water jet cutting

Max thickness 200 mm.
Max length 8,000 mm.

Laser cutting pipe

Max length 15,500 mm.
Max diameter Ø508 mm.

Press bending

Max ton 4,000.
Max working length 21,000 mm.

Find out more

Roll forming

High strength steel.

Find out more

Plate roll bending

Max width 4,500 mm.
Max thickness 110 mm.

Drilling

Max drill bits 70 mm diameter.

Find out more

Milling

Max diameter 360 mm.
Depth 8 mm.

Find out more

Bevelling

Max thickness 140 mm.
Max length of bevel 12,000 mm.

Find out more