Ramor® 600

Download data sheet

General Product Description

The ballistic protection steel with extra-high hardness

 

Ramor® 600 is a ballistic protection steel of extra-high hardness, nominal 600 HBW, available in thicknesses of 3.0 ‑6.0 mm (0.118‑0.236″).

 

Ramor® 600 is available as cut-to-length sheet in thicknesses of 3.0 ‑ 6.0 mm (0.118‑0.236″). Delivered in quenched condition, Ramor® 600 is not intended for further heat treatment.

 

Mechanical Properties

Ramor® 600

Thickness
(inmm)
0.118 - 0.2363.0 - 6.0
Hardness
(HBW)
570 - 640

 

Mechanical Testing

 

Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.

Hardness is measured on a milled surface 0.012 - 0.079" below plate surface.

Chemical Composition (heat analysis)

C
(max %)
C
(max %)
0.40
Si
(max %)
0.70
Mn
(max %)
1.5
P
(max %)
0.015
S
(max %)
0.010
Cr
(max %)
1.50
Ni
(max %)
2.50
Mo
(max %)
0.80
B
(max %)
0.005

The steel is grain-refined. Phosphorous and sulphur are not intentionally alloying elements.

Tolerances

More details are given on www.ssab.com.

Thickness

Product Type
Product Type
Sheet
Thickness
(inmm)
0.118 - 0.1573.00 - 4.00
Tolerance
(inmm)
- 0.0 / + 0.0142- 0.0 / + 0.36
Product Type
Product Type
Sheet
Thickness
(inmm)
0.158 - 0.1974.01 - 5.00
Tolerance
(inmm)
- 0.0 / + 0.0157- 0.0 / + 0.40
Product Type
Product Type
Sheet
Thickness
(inmm)
0.198 - 0.2365.01 - 6.00
Tolerance
(inmm)
- 0.0 / + 0.0165- 0.0 / + 0.42

Length and Width

Sheets are delivered with mill edges cut as standard.

  • Tolerances conform to EN 10051 or to SSAB´s standard after agreement.

Shape

Tolerances according to EN 10051.

Flatness

Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10051.

Product Type
Product Type
Sheet
39.370" ruler
(inmm)
0.2366

Surface Properties

According to EN 10163-2 Class B Subclass 3.

Delivery Conditions

Ramor® is delivered in quenched condition.

Copyright 2026