General Product Description

Pre-hardened, precise, predictable steel.

Toolox® 44 is a steel already heat treated to the final properties.Thus saving time, costs and risks associated with heat treatment.

The very high strength is combined with a high and guaranteed toughness as well as an excellent fatigue resistence. Making Toolox® 44 the ideal choice for the most demanding engineering and mould and die applications.

 

Toolox® 44 can be surface hardened with methods like nitriding, laser and induction. Giving the possibilities to even further improve the performance.

Dimension Range

Toolox® 44 is available as plates in thicknesses between 7.874" - 5.118", as forged block in thicknesses between 5.906" - 12.598", and as round bars in diameters between 0.827" - 13.898". Other dimensions can be available on request. For more information concerning dimensions and tolerances, see Toolox® round bars or Toolox engineering & tool steel dimensional program

Mechanical Properties

Product
Product
Plate
Thickness
(inmm)
0.236 - 5.1186.0 - 130.0
Diameter (inmm)
—
Hardness 1)
(HBW)
410 - 475
Yield strength Rp0.2
(min ksiMPa)
1661150
Tensile strength Rm
(min ksiMPa)
1881300
Elongation A5
(min %)
8
Product
Product
Forged block
Thickness
(inmm)
5.906 - 12.598150.0 - 320.0
Diameter (inmm)
—
Hardness 1)
(HBW)
410 - 475
Yield strength Rp0.2
(min ksiMPa)
—
Tensile strength Rm
(min ksiMPa)
—
Elongation A5
(min %)
—
Product
Product
Round bar
Thickness
(inmm)
—
Diameter (inmm)
0.827 - 5.55121.0 - 141.0
Hardness 1)
(HBW)
410 - 475
Yield strength Rp0.2
(min ksiMPa)
1591100
Tensile strength Rm
(min ksiMPa)
1811250
Elongation A5
(min %)
8
Product
Product
Round bar
Thickness
(inmm)
—
Diameter (inmm)
5.591 - 13.898142.0 - 353.0
Hardness 1)
(HBW)
410 - 475
Yield strength Rp0.2
(min ksiMPa)
—
Tensile strength Rm
(min ksiMPa)
—
Elongation A5
(min %)
—

1) Hardness is measured, according to EN ISO 6506-1. The measurement is performed on a milled surface 0.492" below the ordered surface for forged blocks and round bars. Bar hardness is measured with indents positioned as impact test according to EN 10083. For plate the measurment is preformed on a milled surface 0.020" - 0.079" below the surface.

Impact Properties

Product
Product
Plate
Thickness
(inmm)
0.236 - 5.1186.0 - 130.0
Diameter (inmm)
—
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
13 ft-lbs / 68 °F18 J / 20 °C
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
—
Product
Product
Forged block
Thickness
(inmm)
5.906 - 12.598150.0 - 320.0
Diameter (inmm)
—
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
8 ft-lbs / 68 °F11 J / 20 °C
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
—
Product
Product
Round bar
Thickness
(inmm)
—
Diameter (inmm)
0.827 - 5.55121.0 - 141.0
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
—
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
13 ft-lbs / 68 °F18 J / 20 °C
Product
Product
Round bar
Thickness
(inmm)
—
Diameter (inmm)
5.591 - 13.898142.0 - 353.0
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
—
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 2)
8 ft-lbs / 68 °F11 J / 20 °C

1) Impact testing according to EN 10 025, EN ISO 148 with a 0.079" striker.

2) Impact testing according to EN 10083.

Ultrasonic testing

Ultrasonic inspection is carried out according to: EN 10160 for plate, EN 10228-3 for forged blocks and EN 10308 for round bars . All of them with extra demands according to specification SSAB V6.

Tolerances

For more information concerning dimensions and tolerances, see Toolox® dimensional programs or Toolox® Guarantees available at www.ssab.com or www.toolox.com.

Thickness

Tolerances according to Toolox® Thickness Guarantee.

Toolox® Guarantees meets the requirements of EN 10029 Class C, but offers more narrow tolerances for plates.

Thickness tolerances for Toolox® forged blocks are according to 0"/+0.126".

Bar Diameter

Tolerances according to EN 10060.

Length and Width

Length and width tolerances according to EN 10029 for Toolox® plates.

Length tolerances for Toolox® forged blocks are -9.685"/+9.685".

Length tolerances for Toolox® round bar are according to EN 10060 with tolerances -0/+7.874".

Flatness

Tolerances for Toolox® plates are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).

Maximum accepted flatness deviation for Toolox® forged blocks are 0.039"/39.370".

Bar Straightness

Tolerances according to EN 10060, with a maximum allowed deviation of 0.079".

Surface Properties

According to EN 10163-2 Class B, Subclass 3 for Toolox® plate.

Surface condition for Toolox® forged blocks are milled to roughness of max Ra 12.5 um, and oiled as corrosion protection.

Surface condition for Toolox® round bars are turned and oiled.

Delivery Conditions

Quenched and Tempered at a minimum temperature of 1094 °F.

On delivery from SSAB, Toolox® material meet the following specifications:

 

  • Free from mill scale
  • Not repair welded

 

Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.ssab.com.

Recommendations and instructions

Used for

  • Tooling & Engineering
  • High temperatures (up to 590°C)

Available standard

  • EN 10029

High-strength engineering tool steel