Strenx® Tube 700QLH
Download data sheet
Download data sheet
Strenx® Tube 700QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 700 MPa.
Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 700QLH meets or exceeds the requirements of prEN 10210 (2016).
Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed.
Shapes | Circular |
---|---|
Circular (inmm) | 3.000 - 5.23676.1 - 133.0 |
Wall thickness (inmm) | 0.118 - 0.2363.0 - 6.0 |
Mill length (inmm) | 236.200 - 472.4406000 - 12000 |
Outer diameter (inmm) | 0.118" (ft-lbs) | 0.157" (ft-lbs) | 0.197" (ft-lbs) | 0.236" (ft-lbs) |
---|---|---|---|---|
3.000"76.1" | 3.635 | 4.777 | 5.893 | 6.988 |
3.346"85.0" | 4.078 | 5.368 | 5.893 | 7.855 |
3.500"88.9" | 4.273 | 5.361 | 6.988 | 8.264 |
4.000"101.6" | 4.898 | 6.470 | 7.996 | 9.541 |
4.252"108.0" | 5.221 | 6.921 | 8.533 | 10.146 |
4.500"114.3" | 5.530 | 7.324 | 9.071 | 10.750 |
4.764"121.0" | 5.866 | 7.727 | 9.608 | 11.422 |
5.236"133.0" | 6.464 | 8.533 | 10.616 | 12.632 |
Yield strength Rp0.2 (min ksiMPa) |
Tensile strength Rm (ksiMPa) |
Elongation A5 (min %) |
|
---|---|---|---|
Strenx® Tube 700QLH | 101700 | 113 - 135780 - 930 | 14 |
Mechanical properties meet the requirements of prEN 10210 (2016).
Diameter (inmm) | Min impact energy, transverse test, Charpy V 0.393x0.393" test specimen 1) |
---|---|
3.000 - 5.23676.1 - 133.0 | 30 ft-lbs / -40 °F40 J / -40 °C |
1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 0.236". The specified minimum value corresponds to a full-size specimen.
C (max %) |
Si (max %) |
Mn (max %) |
P (max %) |
S (max %) |
Cr (max %) |
Ni (max %) |
Mo (max %) |
B (max %) |
---|---|---|---|---|---|---|---|---|
0.20 | 0.60 | 1.60 | 0.020 | 0.010 | 0.80 | 2.0 | 0.70 | 0.005 |
In addition, boron (B), molybdenum (Mo), nickel (Ni) or copper (Cu) may be used as alloying elements either singly or in combination.
The steel is grain refined.
Wall Thickness (inmm) | 0.118 - 0.2363.0 - 6.0 |
---|---|
Typ CET(CEV) | 0.34 (0.48) |
Characteristic | Circular hollow sectionsTolerances meet or exceed the requirements of EN 10210 |
---|---|
Outside diameter (D) (1 | ±1%, with a minimum of ±0.0197" and a maximum of ±0.394" |
Out-of-roundness | 2%, when D/T ≤ 3.937" |
Thickness (T) | ±10% |
Straightness | 0.20% of total length and 0.118" over any 39.37" length |
Mass per unit length | Individual tube: ±6% |
Mill length | ≥ 236.22": 0/+1.969" |
Exact length | Agreed at the time of enquiry and order |
1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 3.937".
The tubes are plasma welded quenched and tempered.