1) For both longitudinal and transverse direction.
The mechanical properties are tested in the longitudinal direction.
Tolerances according to Strenx® Thickness Guarantees.
Strenx® Thickness guarantees meet the normal thickness tolerance requirements of EN 10131.
Tolerances according to EN 10131.
Narrower tolerances according to the SSAB standard are available on request.
Length tolerances only apply for cut to length sheets.
Tolerances according to Strenx® Flatness Guarantees Class B.
Strenx® Flatness Guarantees offer narrower tolerances compared to EN 10131.
Flatness guarantees only apply for cut to length sheets.
Cold rolled. Strenx® Cold rolled products are available with mill or cut edge.
Strenx® Cold rolled products has good cold forming, welding and cutting performance.
Strenx® Cold rolled products is not suited for applications requiring hot working or heat treatments at temperatures above 356°F, since the material then may lose its guaranteed properties.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
Strenx® 960 CR is a cold-rolled high-strength structural steel with a minimum yield strength of 960 MPa used to produce stronger and lighter structural applications. Strenx® 960 CR comes with the Strenx® guarantees for flatness, thickness and bending properties, ensuring predictable performance in the workshop. The steel is available as thin sheets or coils with thicknesses between 0.8 and 2.1 mm, width up to 1500 mm and length up to 8500 mm.
Get technical adviceShow specs in:
By upgrading from Strenx® 960 CR to Strenx® 1100 CR, you gain almost 15% higher yield strength. This extra strength can be used to make more high performing components and parts or reduce weight. When you like to discuss upgrading, you are always welcome to get in touch with our steel specialists at SSAB Tech Support or SSAB Knowledge Service Center.