General Product Description

Strenx® P700 is a pressure vessel steel with minimum yield strength of 97 - 101 ksi depending on thickness.

Strenx® P700 is available in four grades, which meet and exceed the requirements of P690Q, P690QH, P690QL1 and P690QL2 in EN 10028-6.

Typical applications are demanding loadbearing structures exposed for pressure and elevated temperatures.

Dimension Range

Strenx® P700 is available as plate in thicknesses of 0.157" – 3.937", widths up to 118,11" and lengths up to 575.983". More detailed information on dimensions is provided in the dimension program for Strenx® P700 at www.ssab.com.

Mechanical Properties

Mechanical properties in room temperature (20°C)

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (inmm)
    Yield strength Rp0.2
    (min ksiMPa)
    Tensile strength Rm
    (ksiMPa)
    Elongation A5
    (min %)
    0.157 - 1.9694.0 - 50.0 101700 111 - 136770 - 940 14
    1.972 - 3.93750.1 - 100.0 97670 111 - 136770 - 940 14
    Compare parameters

    Select one parameter to compare

    Comparison

      For transverse test pieces.

      Yield strength

      Minimum yield strength, Rp0.2, in ksi, at elevated temperatures.

      Hide/Show specific columns Edit
      Select columns to display
        Thickness
        (inmm)
        122°F 212°F 302°F 392°F 482°F 572°F
        0.157 - 1.9694.0 - 50.0 97 93 89 86 83 82
        1.972 - 3.93750.1 - 100.0 94 90 86 83 80 79
        Compare parameters

        Select one parameter to compare

        Comparison

          For transverse test pieces according to EN 10028.

          Impact Properties

          Hide/Show specific columns Edit
          Select columns to display
            Min impact energy, transverse test,
            Charpy V 0.393x0.393" test specimen 1)
            Meet or exceed the requirements for
            50 ft-lbs / -4 °F69 J / -20 °C P690Q, P690QH
            50 ft-lbs / -40 °F69 J / -40 °C P690QL1
            20 ft-lbs / -76 °F27 J / -60 °C P690QL2
            Compare parameters

            Select one parameter to compare

            Comparison

              Min impact energy, transverse test,
              Charpy V 0.393x0.393" test specimen 1)
              50 ft-lbs / -4 °F69 J / -20 °C
              Meet or exceed the requirements for
              P690Q, P690QH
              Min impact energy, transverse test,
              Charpy V 0.393x0.393" test specimen 1)
              50 ft-lbs / -40 °F69 J / -40 °C
              Meet or exceed the requirements for
              P690QL1
              Min impact energy, transverse test,
              Charpy V 0.393x0.393" test specimen 1)
              20 ft-lbs / -76 °F27 J / -60 °C
              Meet or exceed the requirements for
              P690QL2

              1) Unless otherwise agreed, transverse impact testing according to 10 028. For thicknesses between 0.236" - 0.469", sub size Charpy V-specimens are used. The specified minimum value is then proportional to the cross-sectional area of the specimen compared to a full-size specimen (0.393" x 0.393").

              Chemical Composition (heat analysis)

              Hide/Show specific columns Edit
              Select columns to display
                C *)
                (max %)
                Si *)
                (max %)
                Mn*)
                (max %)
                P
                (max %)
                S
                (max %)
                Cr*)
                (max %)
                Ni*)
                (max %)
                Mo*)
                (max %)
                B*)
                (max %)
                Ti*)
                (max %)
                V*)
                (max %)
                0.20 0.80 1.70 0.020 0.005 1.50 2.5 0.70 0.005 0.05 0.12
                Compare parameters

                Select one parameter to compare

                Comparison

                  The steel is grain refined. *) Intentional alloying elements.

                  Carbon Equivalent CET(CEV)

                  Hide/Show specific columns Edit
                  Select columns to display
                    Thickness (inmm) 0.157 - 1.1814.0 - 30.0 1.185 - 3.93730.1 - 100.0
                    Max CET(CEV) 0.38 (0.57) 0.39 (0.58)
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      CET and CEV formula

                      Tolerances

                      More details are given in SSAB’s brochure Strenx® Guarantees.

                      Thickness

                      Tolerances according to EN 10029 Class B. More narrow tolerances are available on request.

                      Length and Width

                      Tolerances conform to EN 10029 or to SSAB’s standard after agreement.

                      Shape

                      Tolerances according to EN 10029.

                      Flatness

                      Tolerances according to Strenx® Flatness Guarantee Class C, which are more narrow than EN 10029 Class N.

                      Surface Properties

                      According to EN 10163-2 Class A, Subclass 3.

                      Delivery Conditions

                      The delivery condition is Quenched and Tempered. The plates are delivered with sheared or thermally cut edges. Untrimmed edges after agreement.

                      Delivery requirements can be found in SSAB’s brochure Strenx® Guarantees or on www.ssab.com.

                      Fabrication and Other Recommendations

                      Welding, bending and machining

                      Recommendations are found in SSAB’s brochures at www.ssab.com or consult Tech Support.

                      Strenx® P700 has bending guarantees according to Strenx® Bending Guarantees Class A. Workshop guidelines for Strenx® P700 refer to the same recommendations as for Strenx® 700 E. Strenx® P700 has obtained its mechanical properties by quenching and subsequent tempering. The properties of the delivery condition cannot be retained after exposure to temperatures in excess of 1076°F.

                      Appropriate health and safety precautions must be taken when welding, cutting, grinding or otherwise working on this product. Grinding, especially of primer coated plates, may produce dust with a high particle concentration.