Strenx® Tube 960QLH

Download data sheet

General Product Description

Strenx® Tube 960QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 960 MPa.

 

Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 960QLH meets or exceeds the requirements of EN 10210-3:2020.

 

Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed. 

Dimension Range

Strenx® Tube 960QLH is available at circular shape.

Shapes
Shapes
Shapes
Circular
Circular
Shapes
Shapes
Circular (inmm)
Circular
3.000 - 5.23676.1 - 133.0
Shapes
Shapes
Wall thickness (inmm)
Circular
0.118 - 0.2363.0 - 6.0
Shapes
Shapes
Mill length (inmm)
Circular
236.200 - 472.4406000 - 12000

Circular Dimensions

Outer diameter (inmm)
Outer diameter (inmm)
3.000"76.1"
0.118" (ft-lbs)
3.635
0.157" (ft-lbs)
4.777
0.197" (ft-lbs)
5.893
0.236" (ft-lbs)
6.988
Outer diameter (inmm)
Outer diameter (inmm)
3.346"85.0"
0.118" (ft-lbs)
4.078
0.157" (ft-lbs)
5.368
0.197" (ft-lbs)
5.893
0.236" (ft-lbs)
7.855
Outer diameter (inmm)
Outer diameter (inmm)
3.500"88.9"
0.118" (ft-lbs)
4.273
0.157" (ft-lbs)
5.361
0.197" (ft-lbs)
6.988
0.236" (ft-lbs)
8.264
Outer diameter (inmm)
Outer diameter (inmm)
4.000"101.6"
0.118" (ft-lbs)
4.898
0.157" (ft-lbs)
6.470
0.197" (ft-lbs)
7.996
0.236" (ft-lbs)
9.541
Outer diameter (inmm)
Outer diameter (inmm)
4.252"108.0"
0.118" (ft-lbs)
5.221
0.157" (ft-lbs)
6.921
0.197" (ft-lbs)
8.533
0.236" (ft-lbs)
10.146
Outer diameter (inmm)
Outer diameter (inmm)
4.500"114.3"
0.118" (ft-lbs)
5.530
0.157" (ft-lbs)
7.324
0.197" (ft-lbs)
9.071
0.236" (ft-lbs)
10.750
Outer diameter (inmm)
Outer diameter (inmm)
4.764"121.0"
0.118" (ft-lbs)
5.866
0.157" (ft-lbs)
7.727
0.197" (ft-lbs)
9.608
0.236" (ft-lbs)
11.422
Outer diameter (inmm)
Outer diameter (inmm)
5.236"133.0"
0.118" (ft-lbs)
6.464
0.157" (ft-lbs)
8.533
0.197" (ft-lbs)
10.616
0.236" (ft-lbs)
12.632

Mechanical Properties

Strenx® Tube 960QLH

Yield strength Rp0.2
(min ksiMPa)
140960
Tensile strength Rm
(ksiMPa)
142 - 167980 - 1150
Elongation A5
(min %)
10

Mechanical properties meet the requirements of prEN 10210 (2016).

Impact Properties

Diameter (inmm)
Diameter (inmm)
3.000 - 5.23676.1 - 133.0
Min impact energy, transverse test,
Charpy V 0.393x0.393" test specimen 1)
30 ft-lbs / -40 °F40 J / -40 °C

1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 0.236". The specified minimum value corresponds to a full-size specimen.

Chemical Composition (heat analysis)

C
(max %)
C
(max %)
0.20
Si
(max %)
0.60
Mn
(max %)
1.60
P
(max %)
0.020
S
(max %)
0.010
Cr
(max %)
0.80
Ni
(max %)
0.20
Mo
(max %)
0.70
B
(max %)
0.005

In addition, boron (B), molybdenum (Mo), nickel (Ni) or copper (Cu) may be used as alloying elements either singly or in combination.

The steel is grain refined. 

Carbon Equivalent CET(CEV)

Wall Thickness (inmm)
Wall Thickness (inmm)
Typ CET(CEV)
0.118 - 0.2363.0 - 6.0
0.36 (0.54)

 

Tolerance Circular

Characteristic
Characteristic
Outside diameter (D) (1
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
±1%, with a minimum of ±0.0197" and a maximum of ±0.394"
Characteristic
Characteristic
Out-of-roundness
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
2%, when D/T ≤ 3.937"
Characteristic
Characteristic
Thickness (T)
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
±10%
Characteristic
Characteristic
Straightness
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
0.20% of total length and 0.118" over any 39.37" length
Characteristic
Characteristic
Mass per unit length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
Individual tube: ±6%
Characteristic
Characteristic
Mill length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
≥ 236.22": 0/+1.969"
Characteristic
Characteristic
Exact length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10210
Agreed at the time of enquiry and order

1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 3.937".

 

Delivery Conditions

The tubes are plasma welded quenched and tempered.