    Product Name Dimensions Standards Datasheet
    SSAB Domex Tube 355J2H Circular: 42.4 - 323.9 mm
    Square: 40x40 - 300x300 mm
    Rectangular: 50x30 - 400x200 mm
    Wall Thickness: 2.0 - 12.5 mm
    Circular: 1.67 - 12.75 in
    Square: in
    Rectangular: in
    Wall Thickness: 0.079 - 0.492 in
    EN 10219-1, EN 10219-2
    SSAB Domex Tube Double Grade Circular: 42.4 - 323.9 mm
    Square: 40x40 - 300x300 mm
    Rectangular: 50x30 - 400x200 mm
    Wall Thickness: 2.0 - 12.50 mm
    Circular: 1.67 - 12.75 in
    Square: in
    Rectangular: in
    Wall Thickness: 0.079 - 0.4921 in
    EN 10219-1, EN 10219-2
    SSAB Domex Tube 460MH Circular: 42.4 - 323.9 mm
    Square: 40x40 - 300x300 mm
    Rectangular: 50x30 - 400x200 mm
    Wall Thickness: 2.0 - 12.5 mm
    Circular: 1.67 - 12.75 in
    Square: in
    Rectangular: in
    Wall Thickness: 0.079 - 0.492 in
    EN 10219-1, EN 10219-2
    SSAB Domex Tube 500MH Circular: 42.4 - 323.9 mm
    Square: 40x40 - 300x300 mm
    Rectangular: 50x30 - 400x200 mm
    Wall Thickness: 2.0 - 12.5 mm
    Circular: 1.67 - 12.75 in
    Square: in
    Rectangular: in
    Wall Thickness: 0.079 - 0.492 in
    EN 10219-2, EN 1090-2
    SSAB Domex Tube 550MH Circular: 42.4 - 323.9 mm
    Square: 40x40 - 300x300 mm
    Rectangular: 50x30 - 400x200 mm
    Wall Thickness: 2.0 - 12.50 mm
    Circular: 1.67 - 12.75 in
    Square: in
    Rectangular: in
    Wall Thickness: 0.079 - 0.4921 in
    EN 10219-2, EN 1090-2
    Compare parameters

    Select one parameter to compare

    Comparison

      SSAB Weathering Tubes

      Hide/Show specific columns Edit
      Select columns to display
        Product Name Dimensions Standards Datasheet
        SSAB Weathering Tube 355WH Circular: 42.4 - 323.9 mm
        Square: 40x40 - 300x300 mm
        Rectangular: 50x30 - 400x200 mm
        Wall Thickness: 2.0 - 12.5 mm
        Circular: 1.67 - 12.75 in
        Square: in
        Rectangular: in
        Wall Thickness: 0.079 - 0.492 in
        EN 10219-2, EN 1090-2
        SSAB Weathering Tube 500WH Circular: 42.4 - 323.9 mm
        Square: 40x40 - 300x300 mm
        Rectangular: 50x30 - 400x200 mm
        Wall Thickness: 2.0 - 12.5 mm
        Circular: 1.67 - 12.75 in
        Square: in
        Rectangular: in
        Wall Thickness: 0.079 - 0.492 in
        EN 10219-2
        Compare parameters

        Select one parameter to compare

        Comparison

          Strenx Tubes

          Hide/Show specific columns Edit
          Select columns to display
            Product Name Thickness range (mmin) Circular (mmin) Square (mmin) Rectangular (mmin) Yield strength (min MPaksi) Standards Shapes Datasheet
            Strenx® Tube 700MLH 2.0 - 10.00.079 - 0.393 42.4 - 323.91.669 - 12.752 40x40 - 300x3001.575x1.575 - 11.811x11.811 50x30 - 400x2001.969x1.181 - 15.748x7.874 700101 EN 10219-3 Circular, Rectangular, Square

            Strenx® Tube 700MLH

            Strenx® Tube 700QLH 3.0 - 6.00.118 - 0.236 76.1 - 133.03.000 - 5.236 - - 700101 EN 10210 Circular

            Strenx® Tube 700QLH

            Strenx® Tube 900MH 4.0 - 6.00.157 - 0.236 139.7 - 219.15.500 - 8.626 100x100 - 200x2003.937x3.937 - 7.874x7.874 120x80 - 250x1504.724x3.149 - 9.843x5.906 900130 EN 10219-3 Circular, Rectangular, Square

            Strenx® Tube 900MH

            Strenx® Tube 960MH 4.0 - 6.00.157 - 0.236 139.7 - 219.15.500 - 8.626 100x100 - 200x2003.937x3.937 - 7.874x7.874 120x80 - 250x1504.724x3.149 - 9.843x5.906 960139 EN 10219-3 Circular, Rectangular, Square

            Strenx® Tube 960MH

            Strenx® Tube 960QLH 3.0 - 6.00.118 - 0.236 76.1 - 133.03.000 - 5.236 - - 960140 EN 10210 Circular

            Strenx® Tube 960QLH