Strenx® Tube 700QLH

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    Strenx® Tube 700QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 700 MPa.

    Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 700QLH meets or exceeds the requirements of prEN 10210 (2016).

    Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed. 

    Dimension Range

    Strenx® Tube 700QLH is available at circular shape.
    Hide/Show specific columns Edit
    Select columns to display
      Shapes Circular
      Circular (mm) 76.1 - 133.0
      Wall thickness (mm) 3.0 - 6.0
      Mill length (mm) 6000 - 12000
      Compare parameters

      Select one parameter to compare

      Comparison

        Shapes
        Circular (mm)
        Circular
        76.1 - 133.0
        Shapes
        Wall thickness (mm)
        Circular
        3.0 - 6.0
        Shapes
        Mill length (mm)
        Circular
        6000 - 12000

        Circular Dimensions

        Hide/Show specific columns Edit
        Select columns to display
          Outer diameter (mm) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m)
          76.1 5.41 7.11 8.77 10.4
          85.0 6.07 7.99 8.77 11.69
          88.9 6.36 8.38 10.4 12.3
          101.6 7.29 9.63 11.9 14.2
          108.0 7.77 10.3 12.7 15.1
          114.3 8.23 10.9 13.5 16.0
          121.0 8.73 11.5 14.3 17.0
          133.0 9.62 12.7 15.8 18.8
          Compare parameters

          Select one parameter to compare

          Comparison

            Mechanical Properties

            Hide/Show specific columns Edit
            Select columns to display
              Yield strength Rp0.2
              (min MPa)
              Tensile strength Rm
              (MPa)
              Elongation A5
              (min %)
              Strenx® Tube 700QLH 700 780 - 930 14
              Compare parameters

              Select one parameter to compare

              Comparison

                Mechanical properties meet the requirements of prEN 10210 (2016).

                Impact Properties

                Hide/Show specific columns Edit
                Select columns to display
                  Diameter (mm) Min impact energy for transversal testing,
                  Charpy V 10x10 mm test specimen 1)
                  76.1 - 133.0 40 J / -40 °C
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Diameter (mm)
                    76.1 - 133.0
                    Min impact energy for transversal testing,
                    Charpy V 10x10 mm test specimen 1)
                    40 J / -40 °C

                    1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6 mm. The specified minimum value corresponds to a full-size specimen.

                    Chemical Composition (ladle analysis)

                    Hide/Show specific columns Edit
                    Select columns to display
                      C
                      (max %)
                      Si
                      (max %)
                      Mn
                      (max %)
                      P
                      (max %)
                      S
                      (max %)
                      Cr
                      (max %)
                      Ni
                      (max %)
                      Mo
                      (max %)
                      B
                      (max %)
                      0.20 0.60 1.60 0.020 0.010 0.80 2.0 0.70 0.005
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        In addition, boron (B), molybdenum (Mo), nickel (Ni) or copper (Cu) may be used as alloying elements either singly or in combination.

                        The steel is grain refined. 

                        Carbon Equivalent CET(CEV)

                        Hide/Show specific columns Edit
                        Select columns to display
                          Wall Thickness (mm) 3.0 - 6.0
                          Typ CET(CEV) 0.34 (0.48)
                          Compare parameters

                          Select one parameter to compare

                          Comparison

                            Wall Thickness (mm)
                            Typ CET(CEV)
                            3.0 - 6.0
                            0.34 (0.48)
                            CET and CEV formula

                            Tolerance Circular

                            Hide/Show specific columns Edit
                            Select columns to display
                              Characteristic Circular hollow sections
                              Tolerances meet or exceed the requirements of EN 10210
                              Outside diameter (D) (1 ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                              Out-of-roundness 2%, when D/T ≤ 100
                              Thickness (T) ±10%
                              Straightness 0.20% of total length and 3 mm over any 1 m length
                              Mass per unit length Individual tube: ±6%
                              Mill length ≥ 6000 mm: 0/+50 mm
                              Exact length Agreed at the time of enquiry and order
                              Compare parameters

                              Select one parameter to compare

                              Comparison

                                Characteristic
                                Outside diameter (D) (1
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                                Characteristic
                                Out-of-roundness
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                2%, when D/T ≤ 100
                                Characteristic
                                Thickness (T)
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                ±10%
                                Characteristic
                                Straightness
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                0.20% of total length and 3 mm over any 1 m length
                                Characteristic
                                Mass per unit length
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                Individual tube: ±6%
                                Characteristic
                                Mill length
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                ≥ 6000 mm: 0/+50 mm
                                Characteristic
                                Exact length
                                Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10210
                                Agreed at the time of enquiry and order

                                1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                Delivery Conditions

                                The tubes are plasma welded quenched and tempered.