Strenx® Tube 700MLH

Download data sheet

General Product Description

Strenx® Tube 700MLH is an HF-welded cold-formed structural hollow section made of hot-rolled high-strength steel with a minimum yield strength of 700 MPa. Its high strength combined with naturally stiff form of welded hollow section enables construction of stronger and lighter structures. Strenx® Tube 700MLH meets or exceeds the requirements to EN 10219-3 (2020) and it is CE marked according to EN 1090-2. Typical applications include load-bearing structures in the lifting, handling and transportation segments, especially in conditions that require extremely good toughness.

Strenx® Tube 700MLH is available in circular, square and rectangular shapes. Other shapes and sizes are available upon request.

The maximum length of the tubes is 12-18 meters, depending on the size. Longer or cut-to-length tubes are available upon request.

Hot dip galvanizing Strenx® Tube 700MLH hollow sections may lead to cracking. Please consult SSAB Tech Support prior galvanization.

Dimension Range

Strenx® Tube 700MLH is available at circular, square and rectangular shapes.
Shapes
Shapes
Circular (mmin)
Dimensions
48.3 - 323.91.669 - 12.752
Shapes
Shapes
Square (mmin)
Dimensions
40x40 - 300x3001.575x1.575 - 11.811x11.811
Shapes
Shapes
Rectangular (mmin)
Dimensions
50x30 - 400x2001.969x1.181 - 15.748x7.874
Shapes
Shapes
Wall thickness (mmin)
Dimensions
2.5 - 10.00.098 - 0.393
Shapes
Shapes
Mill length (mmin)
Dimensions
6000 - 12000 / 18000236.220 - 472.440 / 708.660

Other shapes and sizes are available upon request. 

 

Circular Dimensions

Outer diameter (mmin)
Outer diameter (mmin)
48.31.902
2.5 mm (kg/m)
2.82
3.0 mm (kg/m)
3.35
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
60.32.374
2.5 mm (kg/m)
3.56
3.0 mm (kg/m)
4.24
4.0 mm (kg/m)
5.55
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
76.12.996
2.5 mm (kg/m)
—
3.0 mm (kg/m)
5.41
4.0 mm (kg/m)
7.11
5.0 mm (kg/m)
8.77
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
88.93.500
2.5 mm (kg/m)
—
3.0 mm (kg/m)
6.36
4.0 mm (kg/m)
8.38
5.0 mm (kg/m)
10.4
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
101.64.000
2.5 mm (kg/m)
—
3.0 mm (kg/m)
7.29
4.0 mm (kg/m)
9.63
5.0 mm (kg/m)
11.9
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
108.04.252
2.5 mm (kg/m)
—
3.0 mm (kg/m)
7.77
4.0 mm (kg/m)
10.3
5.0 mm (kg/m)
12.7
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
114.34.500
2.5 mm (kg/m)
—
3.0 mm (kg/m)
8.23
4.0 mm (kg/m)
10.9
5.0 mm (kg/m)
13.5
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
121.04.764
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
11.5
5.0 mm (kg/m)
14.3
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
127.05.000
2.5 mm (kg/m)
—
3.0 mm (kg/m)
9.17
4.0 mm (kg/m)
12.1
5.0 mm (kg/m)
15.0
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
139.75.500
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
13.4
5.0 mm (kg/m)
16.6
6.0 mm (kg/m)
19.8
8.0 mm (kg/m)
26.0
10.0 mm (kg/m)
32.0
Outer diameter (mmin)
Outer diameter (mmin)
168.36.626
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
16.2
5.0 mm (kg/m)
20.1
6.0 mm (kg/m)
24.0
8.0 mm (kg/m)
31.6
10.0 mm (kg/m)
39.0
Outer diameter (mmin)
Outer diameter (mmin)
219.18.626
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
26.4
6.0 mm (kg/m)
31.5
8.0 mm (kg/m)
41.7
10.0 mm (kg/m)
51.6
Outer diameter (mmin)
Outer diameter (mmin)
273.010.748
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
33.1
6.0 mm (kg/m)
39.5
8.0 mm (kg/m)
52.3
10.0 mm (kg/m)
64.9
Outer diameter (mmin)
Outer diameter (mmin)
323.912.752
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
47.0
8.0 mm (kg/m)
62.3
10.0 mm (kg/m)
77.4

 

 

Square Dimensions

Height x Width (mmin)
Height x Width (mmin)
40 x 401.575 x 1.575
2.5 mm (kg/m)
2.82
3.0 mm (kg/m)
3.41
4.0 mm (kg/m)
4.20
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
50 x 501.969 x 1.969
2.5 mm (kg/m)
3.60
3.0 mm (kg/m)
4.38
4.0 mm (kg/m)
5.45
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
60 x 602.362 x 2.362
2.5 mm (kg/m)
4.39
3.0 mm (kg/m)
5.35
4.0 mm (kg/m)
6.71
5.0 mm (kg/m)
8.13
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
70 x 702.756 x 2.756
2.5 mm (kg/m)
—
3.0 mm (kg/m)
6.33
4.0 mm (kg/m)
7.97
5.0 mm (kg/m)
9.70
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
80 x 803.150 x 3.150
2.5 mm (kg/m)
—
3.0 mm (kg/m)
7.30
4.0 mm (kg/m)
9.22
5.0 mm (kg/m)
11.3
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
90 x 903.543 x 3.543
2.5 mm (kg/m)
—
3.0 mm (kg/m)
8.27
4.0 mm (kg/m)
10.5
5.0 mm (kg/m)
12.8
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
100 x 1003.937 x 3.937
2.5 mm (kg/m)
—
3.0 mm (kg/m)
9.25
4.0 mm (kg/m)
11.7
5.0 mm (kg/m)
14.4
6.0 mm (kg/m)
17.0
8.0 mm (kg/m)
21.4
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
120 x 1204.724 x 4.724
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
14.3
5.0 mm (kg/m)
17.6
6.0 mm (kg/m)
20.8
8.0 mm (kg/m)
26.4
10.0 mm (kg/m)
31.8
Height x Width (mmin)
Height x Width (mmin)
140 x 1405.512 x 5.512
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
16.8
5.0 mm (kg/m)
20.7
6.0 mm (kg/m)
24.5
8.0 mm (kg/m)
31.4
10.0 mm (kg/m)
38.1
Height x Width (mmin)
Height x Width (mmin)
150 x 1505.906 x 5.906
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
18.0
5.0 mm (kg/m)
22.3
6.0 mm (kg/m)
26.4
8.0 mm (kg/m)
34.0
10.0 mm (kg/m)
41.3
Height x Width (mmin)
Height x Width (mmin)
160 x 1606.299 x 6.299
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
19.3
5.0 mm (kg/m)
23.8
6.0 mm (kg/m)
28.3
8.0 mm (kg/m)
36.5
10.0 mm (kg/m)
44.4
Height x Width (mmin)
Height x Width (mmin)
180 x 1807.087 x 7.087
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
27.0
6.0 mm (kg/m)
32.1
8.0 mm (kg/m)
41.5
10.0 mm (kg/m)
50.7
Height x Width (mmin)
Height x Width (mmin)
200 x 2007.874 x 7.874
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
30.1
6.0 mm (kg/m)
35.8
8.0 mm (kg/m)
46.5
10.0 mm (kg/m)
57.0
Height x Width (mmin)
Height x Width (mmin)
220 x 2208.661 x 8.661
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
39.6
8.0 mm (kg/m)
51.5
10.0 mm (kg/m)
63.2
Height x Width (mmin)
Height x Width (mmin)
250 x 2509.843 x 9.843
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
45.2
8.0 mm (kg/m)
59.1
10.0 mm (kg/m)
72.7
Height x Width (mmin)
Height x Width (mmin)
300 x 30011.811 x 11.811
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
71.6
10.0 mm (kg/m)
88.4

 

 

Rectangular Dimensions

Height x Width (mmin)
Height x Width (mmin)
50 x 301.969 x 1.181
2.5 mm (kg/m)
2.82
3.0 mm (kg/m)
3.41
4.0 mm (kg/m)
4.20
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
60 x 402.362 x 1.575
2.5 mm (kg/m)
3.60
3.0 mm (kg/m)
4.38
4.0 mm (kg/m)
5.45
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
80 x 403.150 x 1.575
2.5 mm (kg/m)
4.39
3.0 mm (kg/m)
5.35
4.0 mm (kg/m)
6.71
5.0 mm (kg/m)
8.13
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
80 x 603.150 x 2.362
2.5 mm (kg/m)
—
3.0 mm (kg/m)
6.33
4.0 mm (kg/m)
7.97
5.0 mm (kg/m)
9.70
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
100 x 503.937 x 1.969
2.5 mm (kg/m)
—
3.0 mm (kg/m)
6.81
4.0 mm (kg/m)
8.59
5.0 mm (kg/m)
10.50
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
100 x 603.937 x 2.362
2.5 mm (kg/m)
—
3.0 mm (kg/m)
7.30
4.0 mm (kg/m)
9.22
5.0 mm (kg/m)
11.30
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
100 x 803.937 x 3.150
2.5 mm (kg/m)
—
3.0 mm (kg/m)
8.27
4.0 mm (kg/m)
10.5
5.0 mm (kg/m)
12.8
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
120 x 604.724 x 2.362
2.5 mm (kg/m)
—
3.0 mm (kg/m)
8.27
4.0 mm (kg/m)
10.5
5.0 mm (kg/m)
12.8
6.0 mm (kg/m)
—
8.0 mm (kg/m)
—
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
120 x 804.724 x 3.150
2.5 mm (kg/m)
—
3.0 mm (kg/m)
9.25
4.0 mm (kg/m)
11.7
5.0 mm (kg/m)
14.4
6.0 mm (kg/m)
17.0
8.0 mm (kg/m)
21.4
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
150 x 1005.906 x 3.937
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
14.9
5.0 mm (kg/m)
18.3
6.0 mm (kg/m)
21.7
8.0 mm (kg/m)
27.7
10.0 mm (kg/m)
33.4
Height x Width (mmin)
Height x Width (mmin)
160 x 806.299 x 3.150
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
14.3
5.0 mm (kg/m)
17.6
6.0 mm (kg/m)
20.8
8.0 mm (kg/m)
26.4
10.0 mm (kg/m)
31.8
Height x Width (mmin)
Height x Width (mmin)
180 x 1007.087 x 3.937
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
16.8
5.0 mm (kg/m)
20.7
6.0 mm (kg/m)
24.5
8.0 mm (kg/m)
31.4
10.0 mm (kg/m)
38.1
Height x Width (mmin)
Height x Width (mmin)
200 x 1007.874 x 3.937
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
18.0
5.0 mm (kg/m)
22.3
6.0 mm (kg/m)
26.4
8.0 mm (kg/m)
34.0
10.0 mm (kg/m)
41.3
Height x Width (mmin)
Height x Width (mmin)
200 x 1207.874 x 4.724
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
19.3
5.0 mm (kg/m)
23.8
6.0 mm (kg/m)
28.3
8.0 mm (kg/m)
36.5
10.0 mm (kg/m)
44.4
Height x Width (mmin)
Height x Width (mmin)
250 x 1009.843 x 3.937
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
26.2
6.0 mm (kg/m)
31.11
8.0 mm (kg/m)
40.23
10.0 mm (kg/m)
—
Height x Width (mmin)
Height x Width (mmin)
250 x 1509.843 x 5.906
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
30.1
6.0 mm (kg/m)
35.8
8.0 mm (kg/m)
46.5
10.0 mm (kg/m)
57.0
Height x Width (mmin)
Height x Width (mmin)
260 x 18010.236 x 7.087
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
39.6
8.0 mm (kg/m)
51.5
10.0 mm (kg/m)
63.2
Height x Width (mmin)
Height x Width (mmin)
300 x 20011.811 x 7.874
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
45.2
8.0 mm (kg/m)
59.1
10.0 mm (kg/m)
72.7
Height x Width (mmin)
Height x Width (mmin)
400 x 20015.7480 x 7.874
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
4.0 mm (kg/m)
—
5.0 mm (kg/m)
—
6.0 mm (kg/m)
—
8.0 mm (kg/m)
71.6
10.0 mm (kg/m)
—

 

 

Mechanical Properties

Strenx® Tube 700MLH

Yield strength Rp0.2
(min MPaksi)
700101
Tensile strength Rm
(MPaksi)
750 - 950109 - 138
Elongation A5 1)
(min %)
10

1) The hollow sections with D/T < 15 (round) or (B + H)/2T < 12,5 (rectangular and square), the minimum value of elongation is reduced by 2.

The mechanical properties for rectangular hollow sections are tested by SSAB on the longer side of the cross section.

Mechanical properties meet the requirements of EN 10219-3 (2020).

Impact Properties

Product
Product
Strenx® Tube 700MLH
Min impact energy for transversal testing,
Charpy V 10x10 mm test specimen 1)
27 J / -50 °C20 ft-lbs / -58 °F

1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6 mm. The specified minimum value corresponds to a full-size specimen.

Chemical Composition (ladle analysis)

C
(max %)
C
(max %)
0.12
Si
(max %)
0.25
Mn
(max %)
2.10
P
(max %)
0.020
S
(max %)
0.010
Nb
(max %)
0.090 1)
V
(max %)
0.20 1)
Ti
(max %)
0.15 1)

1) Sum of Nb, V and Ti = max 0.22%

Chemical composition meets or exceeds the requirements of EN 10219-3 (2020).

In addition, boron (B), molybdenum (Mo), nickel (Ni) or copper (Cu) may be used as alloying elements either singly or in combination.

The steel is grain refined.

Carbon Equivalent CET(CEV)

Wall Thickness (mm)
Wall Thickness (mm)
Typ CET(CEV)
2.5 - 10.00.098 - 0.394
0.24 (0.38)

 

Tolerance Circular

Characteristic
Characteristic
Outside diameter (D) 1)
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
Characteristic
Characteristic
Out-of-roundness
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
2%
Characteristic
Characteristic
Thickness (T)
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
-5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm.
Characteristic
Characteristic
Straightness
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
0.20% of total length and 3 mm over any 1 m length
Characteristic
Characteristic
Mass per unit length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
Individual tube: ±6%
Characteristic
Characteristic
Mill length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
Characteristic
Characteristic
Exact length
Circular hollow sections
Tolerances meet or exceed the requirements of EN 10219
Agreed at the time of enquiry and order

1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

Tolerance Square

Characteristic
Characteristic
Outside dimensions (B, H) 1)
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
When B, H < 100 mm ±1 % minimum ±0.5 mm
When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
When B, H > 200 mm: ±0.6%
Characteristic
Characteristic
Thickness (T)
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
-5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm.
Characteristic
Characteristic
External corner profile
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
When T ≤ 6 mm: 1.6 x T–2.4 x T
When 6 mm < T ≤ 10 mm: 2.0 x T-3.0 x T
Characteristic
Characteristic
Squareness of side
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
90° ±1°
Characteristic
Characteristic
Concavity/convexity
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
0.8%, with a minimum of 0.5 mm
Characteristic
Characteristic
Twist
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
2 mm + 0.5 mm/m
Characteristic
Characteristic
Straightness
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
0.15% of total length and 3 mm over any 1 m length
Characteristic
Characteristic
Mass per unit length
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
Individual tube: ±6%
Characteristic
Characteristic
Mill length
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
Characteristic
Characteristic
Exact length
Square hollow sections
Tolerances meet or exceed the requirements of EN 10219
Agreed at the time of enquiry and order

1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

Tolerance Rectangular

Characteristic
Characteristic
Outside dimensions (B, H) 1)
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
When B, H < 100 mm ±1 % minimum ±0.5 mm
When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
When B, H > 200 mm: ±0.6%
Characteristic
Characteristic
Thickness (T)
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
-5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm.
Characteristic
Characteristic
External corner profile
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
When T ≤ 6 mm: 1.6 x T–2.4 x T
When 6 mm < T ≤ 10 mm: 2.0 x T-3.0 x T
Characteristic
Characteristic
Squareness of side
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
90° ±1°
Characteristic
Characteristic
Concavity/convexity
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
0.8%, with a minimum of 0.5 mm
Characteristic
Characteristic
Twist
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
2 mm + 0.5 mm/m
Characteristic
Characteristic
Straightness
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
0.15% of total length and 3 mm over any 1 m length
Characteristic
Characteristic
Mass per unit length
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
Individual tube: ±6%
Characteristic
Characteristic
Mill length
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
Characteristic
Characteristic
Exact length
Rectangular hollow sections
Tolerances meet or exceed the requirements of EN 10219
Agreed at the time of enquiry and order

1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

Delivery Conditions

The tubes are cold formed and high frequency welded from thermomechanically rolled steel. 

 