General Product Description

Duroxite® 201 is developed for severe wear and impact applications applying specially formulated abrasive materials on Hardox® 450 backing plate. The overlay material is composed of primary chromium-rich carbides and refined multiple-alloy complex carbides dispersed evenly in a ductile eutectic austenite matrix. The additional multi-alloy carbides are harder and finer than the co-existing chromium-rich carbides which interlock between large primary chromium-rich carbides in a matrix.

Key Benefits

  • Hardox® 450 backing withstands plastic deformation better due to its high yield strength flexing back after impact
  • Provides stronger support due to high hardness and better bonding properties between overlay and base steel
  • Better performance for impact situations than Duroxite® 200 at elevated temperatures up to 350° C (660° F), but impact resistance is best at room temperature

Typical Applications

Duroxite® 201 is widely used in many industries including mining, cement and power generation. Some specific applications include:

Hide/Show specific columns Edit
Select columns to display
    Mining Screen plates, loader bucket liners, feeding systems for ball mills, loader bucket liners, bucket lip shrouds, bucket side shrouds, chutes, liner plates and skip liners
    Cement Cement furnace components, sinter plant parts, fan blades, mixer blades, crews, gyratory mantles, coal and cement pulverizer rolls, raw material crushing components, molding panels
    Power Coal discharger chutes
    Compare parameters

    Select one parameter to compare

    Comparison

      Mining
      Screen plates, loader bucket liners, feeding systems for ball mills, loader bucket liners, bucket lip shrouds, bucket side shrouds, chutes, liner plates and skip liners
      Cement
      Cement furnace components, sinter plant parts, fan blades, mixer blades, crews, gyratory mantles, coal and cement pulverizer rolls, raw material crushing components, molding panels
      Power
      Coal discharger chutes

      For more information on applications see the Duroxite™ Product brochure.

      Standard Dimensions

      Hide/Show specific columns Edit
      Select columns to display
        Standard overlay thicknesses
        Metric unit
        6 mm on 6 mm
        10 mm on 10 mm
        6 mm on 20 mm
        6 mm on 25 mm
        6 mm on 32 mm
        Compare parameters

        Select one parameter to compare

        Comparison

          Standard overlay thicknesses

          Metric unit
          6 mm on 6 mm
          Standard overlay thicknesses

          Metric unit
          10 mm on 10 mm
          Standard overlay thicknesses

          Metric unit
          6 mm on 20 mm
          Standard overlay thicknesses

          Metric unit
          6 mm on 25 mm
          Standard overlay thicknesses

          Metric unit
          6 mm on 32 mm

          Other plate sizes and custom thicknesses can be produced upon request.

          Standard plate sizes

          Hide/Show specific columns Edit
          Select columns to display
            Metric unit Imperial unit
            1.85 m x 2.85 m 6.1' x 9.3'
            1.2 m x 2.4 m 4' x 8'
            1.5 m x 3.0 m 5' x 10'
            1.8 m x 3.0 m 6' x 10'
            Compare parameters

            Select one parameter to compare

            Comparison

              Metric unit
              1.85 m x 2.85 m
              Imperial unit
              6.1' x 9.3'
              Metric unit
              1.2 m x 2.4 m
              Imperial unit
              4' x 8'
              Metric unit
              1.5 m x 3.0 m
              Imperial unit
              5' x 10'
              Metric unit
              1.8 m x 3.0 m
              Imperial unit
              6' x 10'

              Standard plate sizes above are available for all standard overlay thicknesses. Other plate sizes and custom thicknesses can be produced upon request.

              Mechanical Properties

              Hide/Show specific columns Edit
              Select columns to display
                Wear properties
                ASTM G65 – Procedure A weight loss 2)
                Number of overlay passes Typical surface hardness1)

                (HRC)
                Typical surface hardness1)

                (HV)
                Surface
                (g max)
                75 % depth of overlay 3)
                (g max)
                Multiple passes 60 - 65 700 - 850 0.12 0.12
                Compare parameters

                Select one parameter to compare

                Comparison

                  1) Surface hardness is measured on machined flat surface just below overlay surface.

                  2) ASTM G65 - Procedure A weight loss, is a standard test measuring sliding abrasion resistance using a dry sand/rubber wheel apparatus. ASTM G65-Procedure A is the most severe test method.

                  3) ASTM G65 - Procedure A weight loss, wear test is conducted at 75% depth of the overlay materials to ensure consistently good wear resistance from the top surface through to the depth of 75% of the overlay.

                  Microstructure

                  The microstructure of Duroxite® 201 contains primary chromium-rich carbides and refined multiple-alloy complex carbides with a typical hardness of 2500 to 3000 HK4) dispersed evenly in a ductile eutectic austenite matrix. The typical volume fraction of primary chromium-rich carbides is maintained between 30 to 40% with 7 to 10% of multi-alloy complex carbides.

                  4) HK is the Knoop microhardness used primarily for very brittle materials or thin sheets.


                  Tolerances

                  Thickness

                  Overall and overlay thickness tolerances can be guaranteed within ±10% of specified thickness.

                  Flatness

                  Plate flatness tolerance can be guaranteed within ±3 mm (±1/8”) over 1.5 m (5’) plate length for plate dimensions equal to or less than 1.5 m (5’) x 3.0 m (10’). For plates greater than 1.5 m (5’) wide by 3.0 m (10’) long, the following flatness guarantees apply.

                  Hide/Show specific columns Edit
                  Select columns to display
                    Standard overlay thicknesses
                    Flatness tolerance over 1.5 m plate length,
                    Metric unit
                    Metric unit 1.8 m x 3.0 m 2.4 m x 3.0 m
                    5 mm on 8 mm 25 41
                    6 mm on 6 mm 25 41
                    10 mm on 10 mm 12 25
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      For custom sizes, please consult your local sales representative or Hardox Wearparts center for flatness guarantees.

                      Delivery Conditions

                      Duroxite® 201 is normally supplied in an as-welded condition, but can also be supplied in a ground condition upon request.

                      Fabrication and Other Recommendations

                      Welding, cutting, forming and machining

                      Recommendations can be found in the Duroxite® Products brochure, or consult your local technical support representative.

                      Safety precautions

                      When welding or cutting Duroxite® products, gases and harmful fumes are produced that are chemically complex and difficult to classify. The major toxic component in the fumes is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.