    General Product Description

     GreenCoat PLX Pro BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

    This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.

    GreenCoat PLX Pro BT color coated steel offers a high level of durability for standing-seam systems. It is highly formable, even by hand, and has practically no spring-back, which allows for very tight folding.

    GreenCoat PLX Pro BT color coated steel offers a coating that is optimized to resist weathering, resulting in excellent corrosion resistance (RC5+). The product possesses excellent gloss retention and color fastness.

    GreenCoat PLX Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

    The reverse side of the sheet is painted with a two-layer Limestone Turquoise color backside coating.

    GreenCoat PLX Pro BT complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    GreenCoat and PLX are trademarks of the SSAB group of companies.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Regular Matt
      Gloss 40 10
      Minimum inner bending radius 1.5 x sheet thickness 1.5 x sheet thickness
      Scratch resistance 35 N 35 N
      Lowest forming temperature -15 °C -15 °C
      UV radiation resistance RUV3 RUV3
      Corrosion resistance 1) RC5+ RC5+
      Stain resistance Very good Very good
      Highest operating temperature 100 °C 100 °C
      Fire classification, EN 13501-1 A2 s1 d0 A2 s1 d0
      Coating thickness, nominal (primer + top coat) 36 µm 36 µm
      Coating structure Structured Structured
      Steel designation PLX 2) PLX 2)
      Yield strength Rp0.2 Typical 160 MPa 160 MPa
      Tensile strength Rm Typical 320 MPa 320 MPa
      Elongation A80 Typical 41 % 41 %
      Zinc coating 350 g/m2 350 g/m2
      Min steel thickness 3) 0.6 mm 0.6 mm
      Steel width 3) 1000 - 1500 mm 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.

        2) PLX fulfills the requirements of EN 10346 DX54D.

        3) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

        33 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat PLX Pro BT

        Nordic White

        RR1H3 / SS0020

        Regular, Matt

        Winter White

        RR20 / SS0005

        Regular

        Snow White

        RR19 / SS0001

        Regular, Matt

        Arctic White

        RR1L6 / SS0002

        Regular

        Polar White

        RR--- / SS6080

        Matt

        Powder White

        RR--- / SS0021

        Regular

        Limestone Grey

        RR268 / SS0022

        Regular, Matt

        Goosewing Grey

        RR2H5 / SS0461

        Regular

        Gravel Grey

        RR--- / SS0241

        Matt

        Quarry Grey

        RR287 / SS0244

        Regular, Matt

        Rock Grey

        RR237 / SS0061

        Regular

        Anthracite Grey

        RR2H8 / SS0087

        Regular, Matt

        Mountain Grey

        RR23 / SS0036

        Regular, Matt

        Summit Grey

        RR--- / SS0454

        Regular

        Cliff Grey

        RR288 / SS0455

        Matt

        Nordic Night Black

        RR33 / SS0015

        Regular, Matt

        Walnut Brown

        RR32 / SS0387

        Regular, Matt

        Acorn Brown

        RR827 / SS0434

        Regular, Matt

        Coffee Brown

        RR820 / SS0384

        Regular, Matt

        Cottage Red

        RR29 / SS0758

        Regular, Matt

        Brick Red

        RR7F2 / SS0742

        Regular, Matt

        Fire Brick Red

        RR7G9 / SS0757

        Matt

        Harvest Yellow

        RR24 / SS0189

        Regular

        Silver Fir Green

        RR5J3 / SS0975

        Regular, Matt

        Leaf Green

        RR594 / SS0874

        Regular, Matt

        Pine Green

        RR11 / SS0830

        Regular

        Olive Leaf Green

        RR5H8 / SS6033

        Matt

        Lake Blue

        RR35 / SS0558

        Regular

        Metallic Silver

        RR40 / SS0045

        Regular, Matt

        Metallic Sterling

        RR974 / SS6045

        Matt

        Metallic Smokey Silver

        RR977 / SS6015

        Matt

        Metallic Dark Silver

        RR41 / SS0044

        Regular, Matt

        Metallic Copper

        RR979 / SS0778

        Regular

        Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Limestone turquoise
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Limestone turquoise
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.