Strenx® 960 CR

Download data sheet

Dimension Range

Strenx® 960 CR is available in thicknesses of 0.80 - 2.10 mm, widths up to 1500 mm and in lengths up to 8.5 meters, when delivered as cut-to-length sheets.

Mechanical Properties

Yield strength Rp0.2
(min MPaksi)
Yield strength Rp0.2
(min MPaksi)
960139
Tensile strength Rm
(MPaksi)
1100 - 1300174 - 203
Elongation A80
(min %)
3
Min. inner bending radius for a 90° bend 1)
(x t)
3.5

1) For both longitudinal and transverse direction.
The mechanical properties are tested in the longitudinal direction.

 

 

 

Chemical Composition (ladle analysis)

C
(max %)
C
(max %)
0.14
Si
(max %)
0.40
Mn
(max %)
2.00
P
(max %)
0.020
S
(max %)
0.010
Al
(min %)
0.015
Nb+Ti
(max %)
0.10

 

 

 

 

 

Carbon Equivalent CET(CEV)

Thickness (mmin)
Thickness (mmin)
Typ CET(CEV)
0.8 - 2.10.028 - 0.083
0.26 (0.38)

 

Tolerances

More details are given in SSAB’s brochure Strenx® Guarantees.

Thickness

Tolerances according to Strenx® Thickness Guarantees.

Strenx® Thickness guarantees meet the normal thickness tolerance requirements of EN 10131.

Length and Width

Tolerances according to EN 10131.

Narrower tolerances according to the SSAB standard are available on request.

Length tolerances only apply for cut to length sheets. 

Flatness

Tolerances according to Strenx® Flatness Guarantees Class B.

Strenx® Flatness Guarantees offer narrower tolerances compared to EN 10131.

Flatness guarantees only apply for cut to length sheets.

Delivery Conditions

Cold rolled. Strenx® Cold rolled products are available with mill or cut edge.

 

Delivery requirements can be found in SSAB’s brochure Strenx® Guarantees or www.ssab.com.

 

Fabrication and Other Recommendations

Welding, bending and machining

Strenx® Cold rolled products has good cold forming, welding and cutting performance.

Strenx® Cold rolled products is not suited for applications requiring hot working or heat treatments at temperatures above 180°C, since the material then may lose its guaranteed properties.

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Strenx® 960 CR high-strength structural steel

Strenx® 960 CR is a cold-rolled high-strength structural steel with a minimum yield strength of 960 MPa used to produce stronger and lighter structural applications. Strenx® 960 CR comes with the Strenx® guarantees for flatness, thickness and bending properties, ensuring predictable performance in the workshop. The steel is available as thin sheets or coils with thicknesses between 0.8 and 2.1 mm, width up to 1500 mm and length up to 8500 mm.

Get technical advice

Show specs in:

MetricImperial

Add 15% strength by upgrading

By upgrading from Strenx® 960 CR to Strenx® 1100 CR, you gain almost 15% higher yield strength. This extra strength can be used to make more high performing components and parts or reduce weight. When you like to discuss upgrading, you are always welcome to get in touch with our steel specialists at SSAB Tech Support or SSAB Knowledge Service Center.

Copyright 2026