In this scenario 1,125 kg of Strenx® 700 high strength steel replaces 1,500 kg of 500 MPa steel in a loader crane. In addition 1,275 kg of 500 MPa steel replaces 1,500 kg of355 MPa steel in the truck chassis. This means a weight reduction, for the upgraded parts, of 25% in the crane and 15% in the truck. In total a weight reduction of 600 kg is achieved, which increased the load capacity, resulting in higher fuel efficiency and transport efficiency.

SSAB EcoUpgraded

Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.

From the CO2 payback time and onwards, every extra hour brings additional savings.

EcoUpgraded logo

Savings on CO₂

SSAB EcoUpgraded Truck with loader crane
Calculation data
Fuel consumption, fully loaded39 litres/km
Fuel consumption, unladen31 litres/km
Machine usage per year100,000 km/year
Distance with maximum load50%
Service lifetime12 years
Maximum payload (before upgrading)13 800 kg
Gross weight (fully loaded)39 000 kg
Weight of original parts3 000 kg
Weight of upgraded parts2 400 kg