SSAB Docol HR100XF is available in thicknesses of 2.0 - 10.0 mm, and in widths up to 1600 mm as coil, slit coil and as cut to length sheets in lengths up to 16000 mm.
Docol HR100XF
The mechanical properties are tested in the transverse direction.
1) If ReH is not applicable then Rp0.2 is used.
Valid in both the longitudinal and transverse direction.
Docol HR100XF
SSAB Docol HR100XF is available with different levels of Si: from max 0.03%, up to max 0.28%. Max Si 0.03% is the standard version that is suitable for hot dip galvanizing with thin Zinc layers, and for products that will not be galvanized. If the material is to be hot-dip galvanized and a thicker Zinc layer is requested, this must be specified at the time of order.
1) The sum of Nb, V and Ti is max 0.22%.
Tolerances according to 1/2 of EN 10051 category D.
Tolerances according to EN 10051.
Tolerance 3mm/m which only apply for cut to length sheets.
According to EN 10163-2 Class A, Subclass 3.
Thermomechanically Rolled. SSAB Docol HR100XF is available in as rolled or pickled surface condition with mill or cut edge.
SSAB Docol HR100XF has good welding, cold forming and cutting performance. SSAB Docol HR100XF is a cold forming steel not suited for heat treatments at temperatures above 580°C since the material then may lose its guaranteed properties.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.