GreenCoat PLX Pro BT
Proven durability that outlasts the harshest weather.
GreenCoat PLX Pro BT colour coated steel is available in regular and matt finishes and offers a wide range of colours inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).
This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.
GreenCoat PLX Pro BT colour coated steel offers a high level of durability for standing-seam systems. It is highly formable, even by hand, and has practically no spring-back, which allows for very tight folding.
GreenCoat PLX Pro BT colour coated steel offers a coating that is optimized to resist weathering, resulting in excellent corrosion resistance (RC5+). The product possesses excellent gloss retention and colour fastness. GreenCoat PLX Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.
The reverse side of the sheet is painted with a two-layer Limestone Turquoise colour backside coating.
GreenCoat PLX Pro BT complies with current REACH regulations and is fully chromate-free.
SSAB’s colour coated steels are all manufactured according to EN 10169.