Duroxite® 400

Download data sheet

General Product Description

Duroxite® 400 is a specially formulated hardfacing overlay pin engineered and designed to withstand severe heat and metal-to-metal wear applications. Its exceptional quality comes from the precise control and selection of raw materials as well as proprietary processing. The maximum working temperature for the product is 480 °C (900 °F). The work-hardening hardness of the Duroxite® overlay pin can reach up to 58 HRC in service. The Duroxite® 400 overlay pin matches with 12% Manganese Bushings. This Bearing System is expected to last longer than traditional hardened surfaces used such as induction heated and quenched 4140 pins.

 

Key Benefits

  • Provides superior wear resistance in overlay and a tough inner core
  • Performs well when torqueing and surface compression are involved
  • Designed to outlast original equipment and manganese pins

 

Typical Applications

Duroxite® 400 was originally developed for dragline bucket components, but has gained wide acceptance in other applications as well. It is also used for heavy mining or industrial equipment, such as dragline shovels, clam shell buckets, sheave pins, backhoe pins, and crusher shafts.

 

Overlay pins can be machined to meet the requirements of any specific application. For more information on applications see the Duroxite® Product brochure.

 

Standard Dimensions

Standard diameters
Metric unit
Standard diameters
Metric unit
For 127 mm
Standard pin length
Metric unit
Up to 1.22 m
Standard diameters
Metric unit
Standard diameters
Metric unit
For 152 - 280 mm
Standard pin length
Metric unit
Up to 2.74 m

 

Mechanical Properties

Number of overlay passes
Number of overlay passes
Multiple passes
Typical as-welded surface hardness1)
(HRC)
52 - 54
Typical as-welded surface hardness1)
(HV)
540 - 570
Work hardening hardness
(HRC)
Up to 58
Work hardening hardness
(HV)
Up to 650

1) Surface hardness is measured on machined flat surface just below overlay surface.

 

Tolerances

Dimensions

Diameter of Duroxite® 400 can be guaranteed within the typical tolerances of ±0.127 mm (±0.005”).

 

Roundness

Roundness tolerance can be guaranteed within ±0.254 mm (±0.010”).

 

Safety precautions

When welding or cutting Duroxite® products, gases and harmful fumes are produced that are chemically complex and difficult to classify. The major toxic component in the fumes is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.