    General Product Description

    Docol 600FB is a modern hot-rolled advanced high strength steel with a matrix of ferrite or strengthened ferrite containing bainite or strengthened bainite and with a refined grain size.

    The steel grade is well suited for cold formed automotive components such as wheels, chassis components and different structural reinforcements. Formability is very good, especially in hole expansion.

    Docol HR440Y580T-FB meets the requirements of HR440Y580T-FB according to VDA 239-100.

    Dimension Range

    Hot rolled / UC: thickness 2.00-4.00 mm, width up to 1600 mm.

    Hot rolled / GI: thickness 2.00-5.00 mm, width up to 1450 mm.

    Slit strip and cut to length sheets are available upon request.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Standard Coating Test direction
      Yield strength Rp0.2
      (MPa)
      Tensile strength Rm
      (MPa)
      Elongation A80
      (min %)
      Elongation A5
      (min %)
      BH2
      (min MPa)
      Docol HR440Y580T FB VDA 239-100 UC, GI* L 440 - 600 580 - 700 15 17 30
      Compare parameters

      Select one parameter to compare

      Comparison

        *Available upon request.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          Coating C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Al
          (%)
          Nb+Ti
          (max %)
          Cr+Mo
          (max %)
          B
          (max %)
          Cu
          (max %)
          Docol HR440Y580T FB UC, GI* 0.18 0.50 2.00 0.050 0.010 0.015 - 2.00 0.15 1.00 0.010 0.20
          Compare parameters

          Select one parameter to compare

          Comparison

            * Available upon request.

            Tolerances

            Hot-rolled (UC): Tolerances in accordance to EN 10051.

            Hot-dip galvanized (GI): Tolerances in accordance to EN 10143.

            Customized dimensional and shape tolerances are available upon request.

            Coatings

            The metal coating options for Docol products include:

            Hot-dip zinc coating (GI) consists almost entirely of zinc (>99%). It is lead free, resulting in a small zinc spangle size. The coating provides good corrosion protection.

            Galvannealed coating (GA) is a zinc-iron alloy coating having an iron content of approximately 10%. Galvannealed is produced by post-heat treatment in continuous hot-dip coating process. Galvannealed provides excellent resistance weldability and corrosion protection of painted products.

            Galfan coating (ZA) is a zinc-aluminium alloy coating having the eutectic composition approximately of 95% Zn and 5% Al. Galfan is produced in continuous hot-dip coating process. Galfan has better anticorrosive and forming properties than conventional hot-dip zinc coating (GI).

            Electrogalvanized coating (EG) is applied continuously by electro deposition. The coating consists of zinc (>99%). Electrogalvanized steel is characterized by its excellent surface quality and uniform coating thickness.

            Grade specific availability of metal coatings for Docol products is given in the Mechanical properties table (Coating).

            Hide/Show specific columns Edit
            Select columns to display
              Coating type Coating class Standard Closest in EN 10346, informative Coating mass per side, single spot test (g/m2) Thickness per side informative (µm)
              GI 40/40 VDA 239-100 Z100 40 - 60 1) 5.6 - 8.5
              GI 50/50 VDA 239-100 50 - 70 1) 7.0 - 9.9
              GI 60/60 VDA 239-100 Z140 60 - 90 8.5 - 12.7
              GI 70/70 VDA 239-100 70 - 100 9.9 - 14.1
              GI 85/85 VDA 239-100 85 - 115 12.0 - 16.2
              GI 115/115 VDA 239-100 Z275 115 - 155 16.2 - 21.8
              GA 40/40 VDA 239-100 ZF100 40 - 60 1) 5.6 - 8.5
              GA 50/50 VDA 239-100 ZF120 50 - 80 7.0 - 11.3
              ZA 95 EN 10346 ZA95 7.0 -
              ZA 130 EN 10346 ZA130 10.0 -
              EG 25/25 EN 10152 12 - 1.7 -
              EG 50/50 EN 10152 29 - 4.1 -
              EG 75/75 EN 10152 47 - 6.6 -
              EG 100/100 EN 10152 65 - 9.1 -
              Compare parameters

              Select one parameter to compare

              Comparison

                Docol metal coated products are available with surface quality for unexposed applications.

                In addition to these coating masses, OEM specific coatings and single sided EG coatings are available upon request.

                1) For hot-dipped (GI, ZA, GA) hot rolled (HR) grades, the coating mass tolerance is increased to 30 g/m² by increasing the upper limit.

                Surface treatments

                Uncoated (UC): available as oiled.

                Hot-dip galvanized (GI): available as oiled and/or chemically passivated.

                All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

                Fabrication and Other Recommendations

                For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                Docol® Ferritic-Bainitic steel product offer

                Docol® 600FB ferritic-bainitic

                Related content