Docol® PHS 1800 press hardening

Download data sheet

General Product Description

Docol PHS 1800 is cold rolled and alloyed with a small percentage of boron to improve hardenability. This steel is specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Docol PHS FH 1800

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
970
Typical tensile strength Rm (MPa)
1070
Typical elongation A80
(%)
4

Docol PHS CR 1800

Standard
SSAB
Condition
As delivered Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
350
Typical tensile strength Rm (MPa)
500
Typical elongation A80
(%)
27

1) Properties depend on the process.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.27 - 0.33
Si
(%)
0.15 - 0.35
Mn
(%)
1.00 - 1.45
P
(max %)
0.025
S
(max %)
0.010
Cr
(max %)
0.35
B
(%)
0.0008 - 0.0050

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

Ver producto

Docol® PHS 1800 press hardening

Ver producto

Docol® PHS 2000 press hardening

Ver producto

Contenido relacionado

Existencias de materiales de prueba

¿Desea descubrir aplicaciones únicas de automoción, probar nuevos métodos de producción o crear componentes más ligeros que ahorren combustible y mejoren la resistencia a los impactos y la sostenibilidad?

Más información

Datos de conformado para aceros AHSS Docol®

Los clientes existentes de Docol® disfrutan de un acceso 24/7 a los datos de conformado que necesita para ayudarle en su selección y simulación de aceros avanzados de alta resistencia para automoción.

Más información
Copyright 2026