Hot-dip coated steel for lightweight vehicles. Docol 600CP is a steel for complex shapes with energy absorbing capability and corrosion resistance. Examples include complex body-in-white (BIW) and other automotive components. Galvanic corrosion protection of these zinc-based coated products makes them ideal for wet area components.

Dimension Range

Cold rolled / GI, GA, ZA: thickness 0.70-2.50 mm, width up to 1520 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Mechanical Properties

Docol CR​350Y​600T-​CP

Standard
SSAB
Coating
GI, GA, ZA
Test direction
L
Yield strength Rp0.2
(MPa)
350 - 500
Tensile strength Rm
(MPa)
600 - 740
Elongation A80 1)
(min %)
16
BH2
(min MPa)
30
Min. inner bending radius for a 90° bend 2)
1.0 x t

1) For GA coatings the minimum elongation value is reduced by 2 units.

2) In some cases tight bending radius may cause micro-cracking of the coating in the bend area. Where design permits, users are encouraged to employ larger radius.

Chemical Composition (ladle analysis)

Docol CR​350Y​600T-​CP

Coating
GI, GA, ZA
C
(max %)
0.18
Si
(max %)
0.80
Mn
(max %)
2.20
P
(max %)
0.050
S
(max %)
0.010
Al
(%)
0.015 - 1.50
Nb+Ti
(max %)
0.15
Cr+Mo
(max %)
1.00
B
(max %)
0.005

Tolerances

Hot-dip galvanized (GI, GA, ZA): Tolerances in accordance to EN 10143.

Customized dimensional and shape tolerances are available upon request.

Coatings

The metal coating options for Docol® products include:

Hot-dip zinc coating (GI) consists almost entirely of zinc (>99%). It is lead free, resulting in a small zinc spangle size. The coating provides good corrosion protection.

Galvannealed coating (GA) is a zinc-iron alloy coating having an iron content of approximately 10%. Galvannealed is produced by post-heat treatment in continuous hot-dip coating process. Galvannealed provides excellent resistance weldability and corrosion protection of painted products.

Galfan coating (ZA) is a zinc-aluminium alloy coating having the eutectic composition approximately of 95% Zn and 5% Al. Galfan is produced in continuous hot-dip coating process. Galfan has better anticorrosive and forming properties than conventional hot-dip zinc coating (GI).

Grade specific availability of metal coatings for Docol® products is given in the Mechanical properties table (Coating).

Coating type
Coating type
GI
Coating class
40/40
Standard
VDA 239-100
Closest in EN 10346, informative
Z100
Coating mass per side, single spot test (g/m2)
40 - 60
Thickness per side informative (µm)
5.6 - 8.5
Coating type
Coating type
GI
Coating class
50/50
Standard
VDA 239-100
Closest in EN 10346, informative
—
Coating mass per side, single spot test (g/m2)
50 - 70
Thickness per side informative (µm)
7.0 - 9.9
Coating type
Coating type
GI
Coating class
60/60
Standard
VDA 239-100
Closest in EN 10346, informative
Z140
Coating mass per side, single spot test (g/m2)
60 - 90
Thickness per side informative (µm)
8.5 - 12.7
Coating type
Coating type
GI
Coating class
70/70
Standard
VDA 239-100
Closest in EN 10346, informative
—
Coating mass per side, single spot test (g/m2)
70 - 100
Thickness per side informative (µm)
9.9 - 14.1
Coating type
Coating type
GI
Coating class
85/85
Standard
VDA 239-100
Closest in EN 10346, informative
—
Coating mass per side, single spot test (g/m2)
85 - 115
Thickness per side informative (µm)
12.0 - 16.2
Coating type
Coating type
GI
Coating class
115/115
Standard
VDA 239-100
Closest in EN 10346, informative
Z275
Coating mass per side, single spot test (g/m2)
115 - 155
Thickness per side informative (µm)
16.2 - 21.8
Coating type
Coating type
GA
Coating class
40/40
Standard
VDA 239-100
Closest in EN 10346, informative
ZF100
Coating mass per side, single spot test (g/m2)
40 - 60
Thickness per side informative (µm)
5.6 - 8.5
Coating type
Coating type
GA
Coating class
50/50
Standard
VDA 239-100
Closest in EN 10346, informative
ZF120
Coating mass per side, single spot test (g/m2)
50 - 80
Thickness per side informative (µm)
7.0 - 11.3
Coating type
Coating type
ZA
Coating class
95
Standard
EN 10346
Closest in EN 10346, informative
ZA95
Coating mass per side, single spot test (g/m2)
—
Thickness per side informative (µm)
7.0 -
Coating type
Coating type
ZA
Coating class
130
Standard
EN 10346
Closest in EN 10346, informative
ZA130
Coating mass per side, single spot test (g/m2)
—
Thickness per side informative (µm)
10.0 -

Docol® metal coated products are available with surface quality for unexposed applications.

In addition to these coating masses, OEM specific coatings are available upon request.

Surface Treatments

Hot-dip galvanized (GI, GA, ZA): available as oiled and/or chemically passivated.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® Complex Phase steel product offer

Docol® 600 CP complex phase

Obtenga más información

Docol® 800CP complex phase

Obtenga más información

Docol® 1000CP complex phase

Obtenga más información

Docol® 1200CP complex phase

Obtenga más información

Contenido relacionado

Existencias de materiales de prueba

¿Desea descubrir aplicaciones únicas de automoción, probar nuevos métodos de producción o crear componentes más ligeros que ahorren combustible y mejoren la resistencia a los impactos y la sostenibilidad?

Más información

Datos de conformado para aceros AHSS Docol®

Los clientes existentes de Docol® disfrutan de un acceso 24/7 a los datos de conformado que necesita para ayudarle en su selección y simulación de aceros avanzados de alta resistencia para automoción.

Más información
Copyright 2026