The ASTM A516 specification is the Standard Specification for Pressure Vessel Plates, Carbon Steel, for Moderate- and Lower-Temperature Service for plates used in pressure vessel applications where excellent notch toughness is required. Four grades having minimum Tensile Strengths ranging of 55 ksi to 70 ksi are available.