GreenCoat Hiarc Max
Proven durability that outlasts the harshest weather.
GreenCoat Hiarc Max colour coated steel is available in regular and matt finishes. It is available in a wide range of colours inspired by Nordic nature.
GreenCoat Hiarc Max is extremely durable (RC5 and Ruv5) and is specifically developed for faҫades and cassettes. However, it can also be used in roofing applications.
GreenCoat Hiarc Max colour coated steel possesses excellent weather resistance properties and tolerates forming well. It offers extremely good corrosion resistance and is well suited for buildings in the harshest environments, like those near a coastline.
Since GreenCoat Hiarc Max products offer a coating containing fluorine, the surface stays cleaner compared to other products. The coating is also easy to clean due to the hard surface.
The reverse side of the sheet is painted with a two-layer grey backside coating.
GreenCoat Hiarc Max complies with current REACH regulations and is fully chromate-free.
SSAB’s colour coated steels are all manufactured according to EN 10169.