Docol 1000DP dual phase automotive steel

Docol® 1000DP

Advanced high-strength DP steel for forming and welding

Docol® 1000DP dual-phase steel is developed for increased safety in cars. Its high strength allows for weight reduction in BIW applications.

This steel undergoes special heat treatment in a continuous annealing line, producing a two-phase structure. Ferrite that imparts unique forming properties represents one phase, and martensite that accounts for the strength represents the other phase.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Cold rolled / UC, EG: thickness 0.50-2.10 mm, width up to 1527 mm.

Cold rolled / GI, GA, ZA: thickness 0.80-2.00 mm, width up to 1460 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards

VDA 239-100:2016

SSAB

Docol 1000DP

Docol 1000DP

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016

SSAB

DATA SHEET