Hardox 450

Hardox® 450

The most popular abrasion-resistant steel with excellent structural properties.

Hardox® 450 is an abrasion-resistant steel with a nominal hardness of 450 HBW. Hardox® 450 combines good bendability and weldability with an option for guaranteed impact toughness (Hardox® 450 Tuf).

The products can be used in many different components and structures that are subject to wear. Hardox® 450, with an extra 50 Brinell hardness over our 400 grade, provides better dent and abrasion resistance as well as longer wear life, so you can achieve even greater savings.

Order trial material Get free technical advice

Hardox® impact test

Dimension Range

Hardox® 450 is available as plate in thicknesses of 3.2 - 130.0 mm, as sheet in thicknesses 2.0 - 8.0 mm and as cold rolled sheet in thicknesses 0.8 - 2.1 mm. For thicknesses over 80 mm the preferred width is 1650 mm. More detailed information on dimensions is provided in the dimension program.

Available Standards

EN 10029

EN 10051

EN 10131

Hardox® 450

Hardox® 450

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Wear Resistant

DIMENSIONS

T: 0.03 - 5.12 Inches

W: Up to 131.89 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10029

EN 10051

EN 10131

DATA SHEET