SSAB Laser® comes in a wide range of structural and cold forming steel grades. It is available as hot rolled plate, hot rolled sheet and cold rolled sheet. Hot rolled sheet is available in as rolled or pickled condition.

Contact sales
SSAB Laser truck

Fast deliveries when you need it

With stock locations in many countries and a large distribution partner network in Europe, we provide a high product availability and fast deliveries.

Download SSAB Laser® Brochure

pdf 128 Kb
Dimensional and shape tolerances cold rolled steel sheets and coils
pdf 416 Kb
SSAB Laser® - Optimized for you and laser cutting
SSAB Laser brochure
Hide/Show specific columns Edit
Select columns to display
    Product Name Dimensions Standards Datasheet
    SSAB Laser® 250C T: 2.0 - 30.0 mm
    W: 1000 - 3300 mm
    L: 1000 - 16000 mm
    T: 0.079 - 1.18 in
    W: 39.37 - 129.9 in
    L: 39.37 - 629.92 in
    EN 10025-2

    SSAB Laser® 250C

    SSAB Laser® 275C T: 2.0 - 30.0 mm
    W: 1000 - 3300 mm
    L: 1000 - 16000 mm
    T: 0.079 - 1.18 in
    W: 39.37 - 129.9 in
    L: 39.37 - 629.92 in
    EN 10025-2

    SSAB Laser® 275C

    SSAB Laser® 355C T: 3.0 - 30.0 mm
    W: 1000 - 3300 mm
    L: 1000 - 16000 mm
    T: 0.12 - 1.18 in
    W: 39.37 - 129.9 in
    L: 39.37 - 629.92 in
    EN 10025-2

    SSAB Laser® 355C

    SSAB Laser® 355MC Plus T: 3.0 - 15.0 mm
    W: 1000 - 1860 mm
    L: 1000 - 16000 mm
    T: 0.12 - 0.591 in
    W: 39.37 - 73.23 in
    L: 39.37 - 629.92 in
    EN 10149-2

    SSAB Laser® 355MC Plus

    SSAB Laser® 355ML Plus T: 8.0 - 30.0 mm
    W: 1000 - 3300 mm
    L: 2000 - 15000 mm
    T: 0.31 - 1.18 in
    W: 39.37 - 129.9 in
    L: 78.74 - 590.55 in
    EN 10025-4

    SSAB Laser® 355ML Plus

    SSAB Laser® 420MC Plus T: 3.0 - 12.0 mm
    W: 1000 - 1860 mm
    L: 1000 - 16000 mm
    T: 0.12 - 0.472 in
    W: 39.37 - 73.23 in
    L: 39.37 - 629.92 in
    EN 10149-2

    SSAB Laser® 420MC Plus

    SSAB Laser® 420ML Plus T: 10.0 - 25.0 mm
    W: 1000 - 3300 mm
    L: 2000 - 15000 mm
    T: 0.394 - 0.984 in
    W: 39.37 - 129.9 in
    L: 78.74 - 590.55 in
    EN 10025-4

    SSAB Laser® 420ML Plus

    SSAB Laser® 460MC Plus T: 3.0 - 12.0 mm
    W: 1000 - 1800 mm
    L: 1000 - 16000 mm
    T: 0.12 - 0.472 in
    W: 39.37 - 70.87 in
    L: 39.37 - 629.92 in
    EN 10149-2

    SSAB Laser® 460MC Plus

    SSAB Laser® 460ML Plus T: 10.0 - 25.0 mm
    W: 1000 - 3300 mm
    L: 2000 - 15000 mm
    T: 0.394 - 0.984 in
    W: 39.37 - 129.9 in
    L: 78.74 - 590.55 in
    EN 10025-4

    SSAB Laser® 460ML Plus

    SSAB Laser® 500MC Plus T: 3.0 - 8.0 mm
    W: 1000 - 1610 mm
    L: 1000 - 16000 mm
    T: 0.12 - 0.31 in
    W: 39.37 - 63.39 in
    L: 39.37 - 629.92 in
    EN 10149-2

    SSAB Laser® 500MC Plus

    SSAB Laser® DC03 T: 0.8 - 3.0 mm
    W: 730 - 1540 mm
    L: 1200 - 8500 mm
    T: 0.03 - 0.12 in
    W: 28.7 - 60.63 in
    L: 47.24 - 334.6 in
    EN 10130