High hardness armor with extraordinary toughness properties.
Armox® 500T is the world’s toughest protection plate, having nominal 500 HBW hardness, for use in vehicles, buildings and many more applications.
Benefits of Armox® 500T include:
It offers vehicle designers new ways to increase protection using lighter weight designs.
Armox® 500T is not intended for further heat treatment.
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.
Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.
Tensile test according to EN ISO 6892 on each heat and thickness under 19.9 mm.
According to EN ISO 10 160 Class E3S3.
1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.
1) For plate thicknesses >70 mm Cr ≤ 1.5 and Ni ≤3.5. The steel is grain-refined. *) Intentional alloying elements.
More details are given in SSAB´s brochure Armox® Guarantees or on www.ssab.com.
According to SSAB´s dimension program.
Tolerances according to EN 10029.
Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).
According to EN 10163-2 Class B Subclass 3.
The delivery condition is QT (Quenched and Tempered).
Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.