Hot rolled plate

Product Name

SSAB Laser® 250C

Dimensions
T: 2.0 - 30.0 mm
W: 1000 - 3300 mm
L: 1000 - 16000 mm
T: 0.079 - 1.18 in
W: 39.37 - 129.9 in
L: 39.37 - 629.92 in
Standards
EN 10025-2
Datasheet
Product Name

SSAB Laser® 275C

Dimensions
T: 2.0 - 30.0 mm
W: 1000 - 3300 mm
L: 1000 - 16000 mm
T: 0.079 - 1.18 in
W: 39.37 - 129.9 in
L: 39.37 - 629.92 in
Standards
EN 10025-2
Datasheet
Product Name

SSAB Laser® 355C

Dimensions
T: 3.0 - 30.0 mm
W: 1000 - 3300 mm
L: 1000 - 16000 mm
T: 0.12 - 1.18 in
W: 39.37 - 129.9 in
L: 39.37 - 629.92 in
Standards
EN 10025-2
Datasheet
Product Name

SSAB Laser® 355ML Plus

Dimensions
T: 8.0 - 30.0 mm
W: 1000 - 3300 mm
L: 2000 - 15000 mm
T: 0.31 - 1.18 in
W: 39.37 - 129.9 in
L: 78.74 - 590.55 in
Standards
EN 10025-4
Datasheet
Product Name

SSAB Laser® 420ML Plus

Dimensions
T: 10.0 - 25.0 mm
W: 1000 - 3300 mm
L: 2000 - 15000 mm
T: 0.394 - 0.984 in
W: 39.37 - 129.9 in
L: 78.74 - 590.55 in
Standards
EN 10025-4
Datasheet
Product Name

SSAB Laser® 460ML Plus

Dimensions
T: 10.0 - 25.0 mm
W: 1000 - 3300 mm
L: 2000 - 15000 mm
T: 0.394 - 0.984 in
W: 39.37 - 129.9 in
L: 78.74 - 590.55 in
Standards
EN 10025-4
Datasheet